MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Mobility and Materials Crastin® S600LF NC010 PBT  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Crastin® S600LF NC010 is an unreinforced, Teflon® PTFE powder lubricated polybutylene terephthalate resin for injection molding.

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.32 g/cc0.0477 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.20 %
@Temperature 23.0 °C
0.20 %
@Temperature 73.4 °F
50% RH; ISO 62, Similar to
Water Absorption at Saturation 0.40 %
@Temperature 23.0 °C
0.40 %
@Temperature 73.4 °F
By immersion; ISO 62, Similar to
Linear Mold Shrinkage, Flow 0.022 cm/cm
@Thickness 2.00 mm
0.022 in/in
@Thickness 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.022 cm/cm
@Thickness 2.00 mm
0.022 in/in
@Thickness 0.0787 in
ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 58.0 MPa
@Temperature 23.0 °C
8410 psi
@Temperature 73.4 °F
ISO 527
Elongation at Break  15 %
@Temperature 23.0 °C
15 %
@Temperature 73.4 °F
nominal; ISO 527
 25 %
@Temperature 23.0 °C
25 %
@Temperature 73.4 °F
50mm/min; ISO 527
Elongation at Yield 7.5 %
@Temperature 23.0 °C
7.5 %
@Temperature 73.4 °F
ISO 527
Tensile Modulus 2.70 GPa
@Temperature 23.0 °C
392 ksi
@Temperature 73.4 °F
ISO 527
Flexural Strength 80.0 MPa
@Temperature 23.0 °C
11600 psi
@Temperature 73.4 °F
ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²
@Temperature 23.0 °C
1.90 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched  10.0 J/cm²
@Temperature -30.0 °C
47.6 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 14.5 J/cm²
@Temperature 23.0 °C
69.0 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.300 J/cm²
@Temperature -30.0 °C
1.43 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.400 J/cm²
@Temperature 23.0 °C
1.90 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 225 °C437 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 150 °C302 °FISO 75-1/-2
 185 °C365 °FAnnealed; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C131 °FISO 75-1/-2
Flammability, UL94 HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
IEC 60695-11-10
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 °C482 °FOptimum
 240 - 260 °C464 - 500 °F
Mold Temperature 80.0 °C176 °Foptimum
 30.0 - 130 °C86.0 - 266 °F
Drying Temperature 110 - 130 °C230 - 266 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Moisture Content <= 0.040 %<= 0.040 %
 
Descriptive Properties
AdditiveLubricant
 Lubricant, PTFE
AppearanceNatural Color
Drying RecommendedYes
FeaturesChemical Resistance, Good
 Dimensional Stability, Good
 Friction, Low
 Moisture Absorption, Low
 Processability, Good
 Wear Resistance, Good
GenericPBT
Material StatusCurrent
Part Marking Code>PBT<ISO 11469
Polymer FamilyPolyester
Polymer TypePBT
Processing MethodInjection Molding
Product CategoryLow Wear and Friction Resins
 Unreinforced Resins
Resin IdentificationPBTISO 1043
Ultrasonic WeldableYes
UsesParts, Machine/Mechanical

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® A3WG6 30% Glass Filled PA66 (Conditioned)
Covestro Bayblend® T85 XF Polycarbonate + ABS
Covestro Makrolon® 2407 Polycarbonate, Injection Grade
LG Chemical IH830 PMMA, General Purpose Grade for Injection Molding
Celanese Crastin® CE2055 BK580 Polybutylene Terephthalate (PBT)

PZDSZ1047 / 139864

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.