MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Armacell AP Armaflex® Insulation Tape
Categories: Polymer; Adhesive

Material Notes: The mold resistant, elastomeric, AP/Armaflex pressure sensitive insulation tape that provides a fast, easy method of insulating pipes and fittings
  • High-quality AP/Armaflex insulation
  • Fast on difficult pipes and fittings
  • Controls condensation and heat loss
  • Clean, smooth appearance

Information provided by Armacell®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0360 W/m-K
@Temperature 24.0 °C
0.250 BTU-in/hr-ft²-°F
@Temperature 75.2 °F
ASTM C177 or C518
 0.0370 W/m-K
@Temperature 32.0 °C
0.257 BTU-in/hr-ft²-°F
@Temperature 89.6 °F
ASTM C177 or C518
Maximum Service Temperature, Air 82.0 °C180 °FASTM C534
Minimum Service Temperature, Air -183 °C-297 °FASTM C534
Flame Spread Index 2525ASTM E84
 
Descriptive Properties
Bacterial ResistancePassedASTM G22
Fungi ResistancePassedASTM G21/C1338
Mold GrowthPassedUL181
Smoke Developed Index50ASTM E84
Water Vapor Permeability0.05 perm-inASTM E96, Procedure A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Thermal Ceramics Min-K Moldable
3M 856 General Purpose Polyester Tape

PARMD028 / 186639

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.