MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Mobility and Materials VTR 8655 (GBL-S), VTR 8650 8655/8650 Blend  (discontinued **)
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: VTR-8655 is a 68% fluorine, peroxide-cured, Viton® polymer similar to VTR-8650 but with a significantly lower gum polymer viscosity of ~25 (ML at 121°C). VTR-8655 utilizes Advanced Polymer Architecture technology which includes a new peroxide cure site along with an optimized molecular weight distribution designed to deliver a polymer which:
  • Is ideal for blending with VTR-8650 to reach intermediate viscosity ranges
  • Cures exceptionally fast to a high state of cure
  • Shows improved mold release/mold fouling properties compared to Viton® GBL-200
  • Shows improved mold flow and less shear sensitivity than 65 Mooney VTR-8650
  • Shows excellent physical properties with high elongation, both original and aged
  • Shows similar heat, fluids, and low temperature resistance compared to Viton® GBL-200
  • Shows improved water resistance/volume swell in water compared to Viton® GBL-200
  • Shows excellent compression set resistance with either low or no postcure

VTR-8650 is 68% fluorine peroxide cured polymer similar to Viton® GBL-900 but with significantly improved processing and curing characteristics. VTR-8650 utilizes Advanced Polymer Architecture technology which includes a new peroxide cure site along with an optimized molecular weight distribution designed to deliver a polymer which:

  • Cures exceptionally fast to a high state of cure
  • Shows improved mold release/mold fouling properties compared to Viton® GBL-900 and 200
  • Shows improved mold flow, less shear sensitivity, and lower extruder die swell for a ~65 Mooney FKM
  • Shows excellent physical properties with high elongation, both original and aged
  • Shows similar heat, fluids, and low temperature resistance compared to Viton® GBL-900 and 200
  • Shows improved water resistance/volume swell in water compared to Viton® GBL-900 and 200
  • Shows excellent compression set resistance with either low or no postcure

It is recommended if mixing in an internal mixer to use at least a 70% load factor. The recommended process aid for VTR-8650 is 0.5 phr of Armeen® 18D.

Information provided by manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070Cured 7 min at 177°C and Post Cured 2 hr at 232°C
Tensile Strength, Ultimate 20.1 MPa2920 psiCured 7 min at 177°C and Post Cured 2 hr at 232°C
Tensile Strength, Yield 0.800 MPa116 psi10% Modulus, Cured 7 min at 177°C and Post Cured 2 hr at 232°C
Elongation at Break 317 %317 %Cured 7 min at 177°C and Post Cured 2 hr at 232°C
100% Modulus 4.40 MPa
@Strain 100 %
638 psi
@Strain 100 %
Cured 7 min at 177°C and Post Cured 2 hr at 232°C
Compression Set 14 %
@Temperature 200 °C
14 %
@Temperature 392 °F
Method B, O-rings 22 hr at 200°C (Post Cured 4 hr at 232°C)
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -18.1 °C-0.580 °FMDSC, postcured
 
Component Elements PropertiesMetricEnglishComments
Fluorine, F 68 %68 %
 
Descriptive Properties
Formulation as Tested2Varox® DBPH-50
 3Zinc Oxide
 3Diak™ 7 (TAIC)
 30N990 Carbon Black
 50VTR 8655
 50VTR 8650

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials VTR GLT Peroxide Cured Fluoroelastomer (FKM) Formulation
DuPont Mobility and Materials VTR 8655 (GBL-S) Peroxide Cured Fluoroelastomer (FKM)
DuPont Mobility and Materials VTR 8600 (GF-S) Peroxide Cured Fluoroelastomer (FKM)

PDVDA61 / 34030

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.