Buna® SB 1502 - Schkopau is manufactured by cold polymerization using mixed rosin acid / fatty acid soaps. A non-discoloring stabilizer is added during the production process. Buna® SB 1502 - Schkopau is a general purpose rubber. It can be processed in all sectors of the tire and rubber industry. It is mainly used for the production of light-colored rubber articles which can also be applied in the food industry. It is supplied in bales weighing 25 kg. Bales are wrapped in 50 micron PE film. At mixing temperatures above 115°C, the rubber can be processed with the packaging film. Information provided by Dow |