MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Bakelite® PF 7582 Phenolic Molding Compound
Categories: Polymer; Thermoset; Phenolic

Material Notes: Phenolic molding compound, inorganically/organically filled, modified with graphite, good heat conductivity, good sliding properties, high dimension stability.

Applications: modified with graphite, good heat conductivity, good sliding properties, high dimension stability, gas meter valves and grids

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.60 g/cc0.0578 lb/in³ISO 1183
Apparent Bulk Density 0.780 g/cc0.0282 lb/in³ISO 60
Linear Mold Shrinkage 0.0025 cm/cm0.0025 in/inCompression Molding. Post Shrinkage = 0.15%.; ISO 2577
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 80.0 MPa11600 psiISO 178
Flexural Modulus 13.0 GPa1890 ksiISO 178
Charpy Impact Unnotched 0.350 J/cm²1.67 ft-lb/in²ISO 179-1 eU
Charpy Impact, Notched 0.120 J/cm²0.571 ft-lb/in²ISO 179-1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 8.0 MPa 180 °C356 °FISO 75-2
 
Descriptive Properties
Water absorption (mg)824h / 23°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bakelite® PF 6510 Phenolic Molding Compound
Solvay LTM® 10 Epoxy Resin
Röhm Plexiglas® 75 Resist® Extruded Acrylic
Bakelite® PF 7596 Phenolic Molding Compound
Bakelite® PF 7590 Phenolic Molding Compound

PBAKE989 / 192351

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.