MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SunChemical Gwent P2121112P7 Acid Vapor Plasma Modified Multiwalled Carbon Nanotubes
Categories: Carbon

Material Notes: Production Method: CVD
Color: Black
Trial product which has not yet been extensively tested.

Information provided by Gwent Electronic Materials Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.190 g/cc0.00686 lb/in³EN ISO 60
Density 1.70 - 1.90 g/cc0.0614 - 0.0686 lb/in³theoretical
Specific Surface Area 70 - 80 m²/g70 - 80 m²/gBET Analysis
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 98.88 %98.88 %XPS
Oxygen, O 1.12 %1.12 %XPS
 
Descriptive Properties
Acid Number, KOH/mg23titration
Nanotube Length, nm1000SEM
Nanotube Outer Diameter, nm1-5SEM
Zeta Potential, mV28LDE

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Calcium Hydroxyapatite, Ca10(PO4)6(OH)2
SunChemical Gwent P2121112P10 Ammonia Plasma Modified Multiwalled Carbon Nanotubes
SunChemical Gwent P2121112P11 Oxygen Plasma Modified Multiwalled Carbon Nanotubes
SunChemical Gwent P2121112P18 Nitrogen Plasma Modified Multiwalled Carbon Nanotubes
SunChemical Gwent P2121112P8 Argon Plasma Modified Multiwalled Carbon Nanotubes

WGELZ9093 / 139406

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.