MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Forever Plast Namtene® Recycled Standard HDPE
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Standard Namtene® is used for dimple sheet, plastic slabs, and agricultural and construction applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.947 - 0.960 g/cc0.0342 - 0.0347 lb/in³ASTM D792
Melt Flow  0.20 - 0.35 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.20 - 0.35 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 1.2 - 1.6 g/10 min
@Load 5.00 kg,
Temperature 190 °C
1.2 - 1.6 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Ash >= 1 %>= 1 %1 hr; 625°C
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break >= 400 %>= 400 %ASTM D638
Tensile Modulus >= 1.00 GPa>= 145 ksiASTM D638
Flexural Modulus >= 0.900 GPa>= 131 ksiASTM D790
Izod Impact, Unnotched >= 2.70 J/cm>= 5.06 ft-lb/inASTM D256
 
Descriptive Properties
ColorLight Grey, Green, or Black
FormPellets
PP Content< 10%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem Green PE SHC7260 Injection Molding High Density Polyethylene
RTP Company RTP 799 X 140537 High Density Polyethylene (HDPE); Cellulose Fiber - 95% Renewable Resource Content
MBA Polymers HDPE 1107 E Post-consumer recycled fractional melt high density polyethylene
Formosa Plastics Formolene® HB5502Z Blow Molding HDPE
Forever Plast Namtene® 1002 Recycled Pipe Grade HDPE

PFOREV95 / 109556

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.