MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Schott N-BAF10 Glass
Categories: Ceramic; Glass

Material Notes:

Information Provided by SCHOTT North America, Inc.

Key Words: 670471.375
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.75 g/cc0.135 lb/in³
 
Chemical PropertiesMetricEnglishComments
Acid Class, SR 4.34.3
Alkali Class, AR 1.31.3
Stain Resistance Class, FR 0.000.00
 
Mechanical PropertiesMetricEnglishComments
Knoop Microhardness 620620.1/20
Modulus of Elasticity 89.0 GPa12900 ksi
Poissons Ratio 0.2710.271
Shear Modulus 35.0 GPa5080 ksicalculated
 
Thermal PropertiesMetricEnglishComments
CTE, linear  6.20 µm/m-°C
@Temperature -30.0 - 70.0 °C
3.44 µin/in-°F
@Temperature -22.0 - 158 °F
 7.00 µm/m-°C
@Temperature 20.0 - 300 °C
3.89 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.560 J/g-°C0.134 BTU/lb-°F
Thermal Conductivity 0.780 W/m-K5.41 BTU-in/hr-ft²-°F
Transformation Temperature, Tg 660 °C1220 °F
Softening Point 790 °C1450 °FViscosity 107.6 dPa s
Annealing Point 652 °C1210 °FViscosity 1013.0 dPa s
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.67003
@Wavelength 587.6 nm
1.67003
@Wavelength 587.6 nm
nd
 1.67341
@Wavelength 546.1 nm
1.67341
@Wavelength 546.1 nm
ne
Abbe Number 46.8346.83ve
 47.1147.11vd
Optical Dispersion 0.0142220.014222nf - nc
 0.014380.01438nf' - nc'
Transmission, Visible  84.7 %
@Thickness 10.0 mm,
Wavelength 380 nm
84.7 %
@Thickness 0.394 in,
Wavelength 380 nm
 95.9 %
@Thickness 10.0 mm,
Wavelength 405 nm
95.9 %
@Thickness 0.394 in,
Wavelength 405 nm
 98.7 %
@Thickness 10.0 mm,
Wavelength 460 nm
98.7 %
@Thickness 0.394 in,
Wavelength 460 nm
 99.6 %
@Thickness 10.0 mm,
Wavelength 580 nm
99.6 %
@Thickness 0.394 in,
Wavelength 580 nm
 99.8 %
@Thickness 10.0 mm,
Wavelength 700 nm
99.8 %
@Thickness 0.394 in,
Wavelength 700 nm
IR Transmittance  72.7 %
@Thickness 10.0 mm,
Wavelength 2500 nm
72.7 %
@Thickness 0.394 in,
Wavelength 2500 nm
 99.2 %
@Thickness 10.0 mm,
Wavelength 1530 nm
99.2 %
@Thickness 0.394 in,
Wavelength 1530 nm
UV Transmittance  17.6 %
@Thickness 10.0 mm,
Wavelength 350 nm
17.6 %
@Thickness 0.394 in,
Wavelength 350 nm
 62.6 %
@Thickness 10.0 mm,
Wavelength 365 nm
62.6 %
@Thickness 0.394 in,
Wavelength 365 nm
 72 %
@Thickness 10.0 mm,
Wavelength 370 nm
72 %
@Thickness 0.394 in,
Wavelength 370 nm
 
Descriptive Properties
B1
Climatic Resistance Test CR1
HG4
K (10-6mm2/N)2.37
Phosphate Resistance PR1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Schott N-SF11 Glass
Ohara L-LAL12 Low Tg Optical Glass
Ohara S-LAL12 Optical Glass
Schott SF11 785258.474, Optical Glass
Schott N-SF10 Glass

CSGS042 / 93376

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.