MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Westlake Tymax® GT7058 Anhydride Modified Acrylate Copolymer
Categories: Polymer; Thermoplastic; Polyethylene (PE); Anhydride-Modified Polyethylene

Material Notes: Westlake GT7058 is an anhydride modified acrylate copolymer designed for blown film extrusion that contains no slip and no antiblock additives. This resin is designed to function as a coextruded tie layer in multilayer film applications. Westlake GT7058 is designed to tie polyethylene to resins that typically have poor bonding characteristics such as polyamide and EVOH. Its applications include: blown film, packaging, and tie-layer.

Information provided by Westlake Chemical Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.943 g/cc0.0341 lb/in³ASTM D4883
Methyl Acrylate Content 24 %24 %Westlake
Melt Flow 2.7 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.7 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Thermal PropertiesMetricEnglishComments
Melting Point 74.0 °C165 °FDSC; ASTM D3418
Crystallization Temperature 43.0 °C109 °FDSC; ASTM D3418

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Lucalen A2920M Low Density Polyethylene
LyondellBasell Lucalen A2540D Low Density Polyethylene
LyondellBasell Lucalen A2700H Low Density Polyethylene
LyondellBasell Lucalen A2700M Low Density Polyethylene
LyondellBasell Lucalen A2910M Low Density Polyethylene

PWESF9006 / 106843

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.