MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ATI Allvac® Nickelvac® 400 UNS N04400 Nickel Superalloy
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Nickel-Copper solid solution alloy. Uses: Equipment for mineral acids, brines, alkalis, offshore engineering, marine applications.

Property values are for samples in the metallurgical condition: 1650°F anneal.

Information provided by Allvac, An Allegheny Teledyne Company.

Key Words: AMS 4675, 4730. ASTM B 127, B 164, B 564
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.83 g/cc0.319 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 7070
Tensile Strength, Ultimate 551 MPa79900 psi
Tensile Strength, Yield 241 MPa
@Strain 0.2 %
35000 psi
@Strain 0.2 %
Elongation at Break 40 %40 %
Reduction of Area 70 %70 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.15 %0.15 %
Copper, Cu 31 %31 %
Iron, Fe 1.2 %1.2 %
Manganese, Mn 1.0 %1.0 %
Nickel, Ni 66 %66 %
Silicon, Si 0.25 %0.25 %
Sulfur, S 0.010 %0.010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Special Metals MONEL® Alloy 400
Carlson C 400 Nickel-Copper Alloy
ATI Allvac® 520 Nickel Superalloy, Heat Treatment: 1121°C (2050°F) + Age
ATI Allvac® Nickelvac® C 22 UNS N06022 Nickel Superalloy
ATI Allvac® Nickelvac® C-276 UNS N10276 Nickel Superalloy

NALLV00 / 14916

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.