MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Pinnacle Polymers 1703 Polypropylene Homopolymer, Stretched Tape Grade
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Fiber Grade

Material Notes: This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties and lot-to-lot consistency.

Features:

  • Excellent color and processing stability
  • Resistance to gas fading
  • Low water carry-over
  • Excellent lot-to-lot consistency

Applications:

  • Woven products
  • Carpet backing
  • Sacking
  • Industrial and geotextile fabrics

Certifications: Pinnacle's polypropylene, as marketed by Pinnacle Polymers Company, in natural, uncolored pellet form complies with appropriate requirements of CFR Title 21, Part 177, Subpart B, Section 177.1520 (c) 1.1a entitled “Olefin Polymers” of the Food Additives Amendment of 1958 to the United States Food, Drug and Cosmetic Act of 1938.

Information provided by Pinnacle Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Melt Flow 3.5 g/10 min3.5 g/10 minCondition L 230/2.16; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 35.9 MPa
@Thickness 3.20 mm
5200 psi
@Thickness 0.126 in
At 51mm/min, injection molded ASTM Type 1 specimen; ASTM D638
Elongation at Yield 10 %
@Thickness 3.20 mm
10 %
@Thickness 0.126 in
At 51mm/min, injection molded ASTM Type 1 specimen; ASTM D638
Flexural Modulus, 1% Secant 1650 MPa
@Thickness 3.20 mm
240000 psi
@Thickness 0.126 in
At 1.27 mm/min, injection molded ASTM Type 1 specimen; ASTM D790A
Izod Impact, Notched 0.374 J/cm
@Thickness 3.20 mm,
Temperature 22.8 °C
0.700 ft-lb/in
@Thickness 0.126 in,
Temperature 73.0 °F
injection molded ASTM Type 1 specimen; ASTM D256
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pinnacle Polymers 1508 Polypropylene Homopolymer, Fiber Spinning Grade
Total PPR 7450HC Polypropylene, Film Extrusion Grade
Total PPR 6827MZ Polypropylene, Random Copolymer - High Flow Clarified - for Injection Molding
Total PPH 3860X Polypropylene Homopolymer, High Flow Reactor Grade for Non-Woven Fibers
Pinnacle Polymers 1704 Polypropylene Homopolymer, Stretched Tape Grade

PPINN12 / 56265

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.