MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trelleborg P600 Epichlorohydrin
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: There are three types of epichlorohydrin:
1. Homopolymers of epichlorohydrin. Designated CO.
2. Chopolymers of epichlorohydrin and etylene oxide. Designated ECO.
Terpolymers of epichlorohydrin, etylene oxide and a unsaturated monomer make it possible to vulcanize using sulphur. Designated GECO.

    Properties
  • Excellent resistance to ozone and weathering.
  • Good high temperature resistance.
  • Reasonable low temperature resistance.
  • Very low permeability to gases -- even better than Butyl rubber.
  • Good fire resistance.
  • Excellent elasticity.
  • Resistance to Chemicals; resistant to hydrocarbon products. Their good oil resistance properties are very similar to those of medium to high Nitrile grades. Superior resistance to aromatic hydrocarbons. Reasonable resistance to alcohol, alkalies and diluted mineral acids. Limited resistance to most organic chemical products and are not recommended for use with oxidizing agents and chlorine.

All information provided by Trelleborg

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.39 g/cc1.39 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060
Tensile Strength, Yield 10.5 MPa1520 psi
Elongation at Break 300 %300 %
Compression Set 25 %
@Temperature 100 °C,
Time 79200 sec
25 %
@Temperature 212 °F,
Time 22.0 hour
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 135 °C275 °F
Minimum Service Temperature, Air -35.0 °C-31.0 °F
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trelleborg P650 Epichlorohydrin
Armacell Monarch® F-05013 (Black) Neoprene, EPDM, SBR Blend Foam
3M Dyneon™ PVDF 32008/0009 Polyvinylidene Fluoride
Epichlorohydrin Rubber (CO, ECO)
Dow Buna® SB 1500 Cold polymerized Emulsion Styrene Butadiene Rubber (E-SBR)

PTRELL161 / 83919

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.