MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

High Silicon Ductile Iron at RT 4Si nominal alloy content
Categories: Metal; Ferrous Metal; Cast Iron; Alloy Cast Iron; Ductile Iron

Material Notes: Subcritically annealed for 4 hours at 790°C, air cooled.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.10 - 7.20 g/cc0.257 - 0.260 lb/in³Typical value of ductile iron
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 565 MPa81900 psi
 60.0 MPa
@Temperature 700 °C
8700 psi
@Temperature 1290 °F
 80.0 MPa
@Temperature 650 °C
11600 psi
@Temperature 1200 °F
 245 MPa
@Temperature 540 °C
35500 psi
@Temperature 1000 °F
Tensile Strength, Yield 445 MPa
@Strain 0.2 %
64500 psi
@Strain 0.2 %
 50.0 MPa
@Strain 0.2 %,
Temperature 700 °C
7250 psi
@Strain 0.2 %,
Temperature 1290 °F
 65.0 MPa
@Strain 0.2 %,
Temperature 650 °C
9430 psi
@Strain 0.2 %,
Temperature 1200 °F
 225 MPa
@Strain 0.2 %,
Temperature 540 °C
32600 psi
@Strain 0.2 %,
Temperature 1000 °F
Elongation at Break 19.5 %19.5 %
 45 %
@Temperature 540 °C
45 %
@Temperature 1000 °F
 59 %
@Temperature 650 °C
59 %
@Temperature 1200 °F
 87.5 %
@Temperature 700 °C
87.5 %
@Temperature 1290 °F
 
Component Elements PropertiesMetricEnglishComments
Iron, Fe 96 %96 %
Silicon, Si 4.0 %4.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ductile Iron grade 60-40-18
ASTM A439 Austenitic Ductile Iron type D2
Gray Cast Iron, ASTM A 48 Class 40
High Silicon Ductile Iron at RT 4Si-0.9V nominal alloy content
ASTM A439 Austenitic Ductile Iron type D5S

MDFE27 / 12024

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.