MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Hostacom 68F4-3 BLK Polypropylene with 30% Talc Filler
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Talc Filler

Material Notes: Hostacom 68F4-3 BLK fractional melt flow, 3,400 MPa flexural modulus, 30% talc-filled, blow molding and extrusion grade polypropylene homopolymer is typically used for applications that require high strength, stiffness, impact resistance and processability. Applications: Panels & Profiles.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³Method A
Melt Flow 0.50 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.50 g/10 min
@Load 4.76 lb,
Temperature 446 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 33.0 MPa4790 psi
Elongation at Yield 6.0 %6.0 %
Flexural Modulus 3.40 GPa493 ksi
Izod Impact, Notched (ISO) 7.00 kJ/m²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 125 °C257 °Funannealed
 
Descriptive Properties
Processing MethodCompounding, Extrusion Blow Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Hostacom BFT 30 Polypropylene with 30% Talc Filler
LyondellBasell Hostacom EKC 455P G82779 Polypropylene with 30% Talc Filler
LyondellBasell Astryn 65F4-3 Polypropylene Homopolymer, 30% Talc
Washington Penn Homopolymer Polypropylene 30% Talc Filled
Global TPP-130 30% Talc Filled Polypropylene

PEQT7647 / 219284

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.