MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Copper, UNS C18100, Cold Worked (40% reduction) Strip
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Excellent capacity for both cold and hot forming. Excellent solderability. Good brazing and gas-shielded arc welding. Fair butt resistance welding.

Applications: resistance welding electrodes and wheels, switches, circuit breakers, high temperature wire, semiconductor bases, heat sinks, and continuous casting molds.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.88 g/cc0.321 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 460 MPa66700 psi
Tensile Strength, Yield >= 430 MPa>= 62400 psi
Elongation at Break 6.0 %6.0 %in 50 mm
Modulus of Elasticity 125 GPa18100 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000217 ohm-cm
@Temperature 20.0 °C
0.00000217 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.7 µm/m-°C
@Temperature 20.0 - 100 °C
9.28 µin/in-°F
@Temperature 68.0 - 212 °F
 18.4 µm/m-°C
@Temperature 20.0 - 200 °C
10.2 µin/in-°F
@Temperature 68.0 - 392 °F
 19.3 µm/m-°C
@Temperature 20.0 - 300 °C
10.7 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.393 J/g-°C0.0940 BTU/lb-°F
Thermal Conductivity 324 W/m-K2250 BTU-in/hr-ft²-°F
Melting Point <= 1075 °C<= 1967 °F
Liquidus 1075 °C1967 °F
Annealing Point 593 - 704 °C1100 - 1300 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 600 - 700 °C1110 - 1290 °F
Solution Temperature 900 - 975 °C1650 - 1790 °FFor 1 hour
Aging Temperature 400 - 500 °C752 - 932 °FFor 1 hour
Hot-Working Temperature 790 - 925 °C1450 - 1700 °F
 
Component Elements PropertiesMetricEnglishComments
Chromium, Cr 0.40 - 1.2 %0.40 - 1.2 %
Copper, Cu 99 %99 %
Magnesium, Mg 0.030 - 0.060 %0.030 - 0.060 %
Zirconium, Zr 0.050 - 0.30 %0.050 - 0.30 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cartridge Brass, UNS C26000 (260 Brass), OS100 Temper flat products
Chromium Copper, UNS C18400
High Strength Modified Copper, UNS C19400, H14 Temper flat products
MetalTek C18100 Chrome Zirc Copper High Conductivity
Beryllium Copper, UNS C17200, TB00 Temper Strip

MC18100b1 / 10905

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.