Braskem Idealis 500 Compression Molding High Molecular Weight Polyethylene
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Polyethylene (PE)
;
High Density (HDPE)
;
UHMW PE (Ultra High Molecular Weight PE)
Material Notes:
Braskem Idealis 500 is the only high molecular weight polyethylene resin in powder form specially designed for the compression molding process. Its applications range from food handling, cutting boards, and playground toys to technical parts.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.951
g/cc
0.0344
lb/in³
ASTM-D792
Apparent Bulk Density
0.450
g/cc
0.0163
lb/in³
ASTM-D1895
Particle Size
170
µm
170
µm
Average, Dp50; ASTM-D1921
Viscosity Test
470
cm³/g
4.70
dl/g
Intrinsic; ASTM-D4020
Molecular Weight
550000
g/mol
550000
g/mol
Melt Flow
0.70
g/10 min
@Load 21.6 kg,
Temperature 190 °C
0.70
g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM-D1238
Mechanical Properties
Metric
English
Comments
Hardness, Shore D
63
63
15 sec; ASTM-D2240
Tensile Strength at Break
>=
30.0
MPa
>=
4350
psi
ASTM-D638 / ISO 527
Tensile Strength, Yield
>=
20.0
MPa
>=
2900
psi
ASTM-D638 / ISO 527
Elongation at Break
>= 500 %
>= 500 %
ASTM-D638 / ISO 527
Flexural Modulus
0.930
GPa
135
ksi
ASTM-D790
Charpy Impact, Notched
>=
5.00
J/cm²
>=
23.8
ft-lb/in²
double-notched specimens (14° v-notch on both sides); ISO 11542-2
Sand Slurry
80
80
Sand slurry - Internal, reference PE500 = 100
Thermal Properties
Metric
English
Comments
Melting Point
136
°C
277
°F
ASTM-D3418
Vicat Softening Point
80.0
°C
@Load 5.10 kg
176
°F
@Load 11.2 lb
ASTM-D1525
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Braskem UTEC® 3040 Ultra High Molecular Weight Polyethylene
Braskem UTEC® 6541 Ultra High Molecular Weight Polyethylene
Braskem Idealis 500 High Molecular Weight Polyethylene Powder
Braskem UTEC® 4040 Ultra High Molecular Weight Polyethylene
Braskem UTEC® 3041 Ultra High Molecular Weight Polyethylene
PBRAS825 / 106671
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.