Liquid silicone rubbers of the ELASTOSIL® LR 3043 series are paste-like, easily-pigmentable two component compounds with short curing times. Their vulcanizates are noted for their high transparency and excellent mechanical and electrical properties. Properties: The products can be used within a temperature range of - 55°C to + 210°C. The addition of heat stabilizers at service temperatures of more than 180°C is recommended. Application: These grades are particularly suitable for the economical production of large series of injection molded articles. Parts made from ELASTOSIL® LR 3043/40 A/B can be used for technical applications. Postcured parts can be used for applications in the food industries and are suitable for use under the Recommendations "XV. Silicone" of the BfR and FDA § 177.2600. Information provided by Wacker Chemie AG. |