MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman Premi-Glas® 1100-20 Fiberglass Reinforced Thermoset BMC
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset

Material Notes: Premi-Glas® 1100-20 is a fiberglass reinforced thermoset bulk molding compound for general purpose applications requiring thermal stability and stiffness.

Key features and benefits are:

  • Excellent stiffness to weight ratio, non-melting
  • Good dimensional stability, including excellent thermal resistance
  • Pigmentable for molded-in color; best appearance with mold texture
  • Excellent property retention in cold and hot environments
  • Good corrosion resistance except in acid environments.
  • Designed for compression or injection molding in matched metal die molds.

A. Schulman has acquired this former Premix product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.70 - 1.85 g/cc1.70 - 1.85 g/cc
Linear Mold Shrinkage 0.0015 - 0.0035 cm/cm0.0015 - 0.0035 in/inPolymerization Shrinkage
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 31.0 MPa4500 psiASTM D638
Tensile Modulus 14.0 GPa2030 ksiASTM D638
Flexural Strength 110 MPa16000 psiASTM D790
Flexural Modulus 10.0 GPa1450 ksiASTM D790
Poissons Ratio 0.300.30
Shear Modulus 5.40 GPa783 ksiCalculated
Izod Impact, Notched 4.25 J/cm7.96 ft-lb/inASTM D256
Izod Impact, Unnotched 5.30 J/cm9.93 ft-lb/inASTM D4812
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 35.0 µm/m-°C19.4 µin/in-°FZ Direction
CTE, linear, Transverse to Flow 25.0 µm/m-°C13.9 µin/in-°FXY Direction
Thermal Conductivity 0.300 W/m-K2.08 BTU-in/hr-ft²-°F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 150 °C302 °FCompression or Injection Molding
Clamp Pressure 3.45 - 6.89 MPa500 - 1000 psiMolding Pressure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman Premi-Glas® 1100-10 Fiberglass Reinforced Thermoset BMC
A. Schulman Premi-Glas® 1100V-15 Fiberglass Reinforced Thermoset BMC
A. Schulman Premi-Glas® 1100V-20 Fiberglass Reinforced Thermoset BMC
A. Schulman Premi-Glas® 1100V-10 Fiberglass Reinforced Thermoset BMC
A. Schulman Premi-Glas® 1100-25 Fiberglass Reinforced Thermoset BMC

PPREMH943 / 140341

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.