MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Teijin Films Melinex® 813G Polyester Packaging Film, 48 Gauge  (discontinued **)
Categories: Polymer; Film; Renewable/Recycled Polymer; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Data provided by DuPont Packaging Polymers.

Melinex® ECOTM 813G is a clear, pretreated base film with high gloss, low haze and excellent processability. It is produced using a minimum of 25 percent post-consumer recycled feedstock. Melinex® ECOTM 813G polyester film has been designed to provide a clear film with excellent ink adhesion and printability for the packaging industry. One side is a chemically pretreated surface that provides ink adhesion to a wide range of both solvent and water based inks. Melinex® ECOTM 813G film provides good clarity for reverse printing and allows the inks to shine through with high quality.

Melinex® ECOTM 813G film's pretreated surface also provides improved adhesion for various coatings and adhesives. This often eliminates the need for any type of priming operation. The chemical pretreatment on Melinex® ECOTM 813G film does not result in a performance or shelf-life decline over time and generally is superior to corona treated film. Melinex® ECOTM 813G film features good clarity and handling characteristics in metallizing operations. When aluminum metallized, the film exhibits excellent aesthetic quality as well as the best barrier to oxygen and moisture in a flexible packaging film.

Polyester base film, containing a minimum of 25% post consumer recycled polyester content, that is compliant with FDA regulations under 21 CFR 177.1630, Sections (f) and (g), which is treated on one side with a coating which is also in compliance with 21 CFR 177.1630. Melinex® ECOTM813G may be used for packaging, transporting, or holding food, excluding alcoholic beverages, at temperatures not to exceed 250°F, and for packaging, transporting, or holding alcoholic beverages that do not exceed 50 percent alcohol by volume.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³
Moisture Vapor Transmission 0.0120 cc-mm/m²-24hr-atm0.0305 cc-mil/100 in²-24hr-atmmetallized barrier; 2.8 g/100in²-24hr-atm unmetallized barrier; Tested per ASTM F372 at 100°F, 90% RH.
Oxygen Transmission 0.0200 cc-mm/m²-24hr-atm0.0508 cc-mil/100 in²-24hr-atmmetallized barrier; 6 cc/100in²-24hr-atm unmetallized barrier; Tested per ASTM D1434 at 77°F, 75% RH.
Thickness 12.2 microns0.480 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 105 %105 %ASTM D882A
Film Elongation at Break, TD 60 %60 %ASTM D882A
Coefficient of Friction, Dynamic 0.400.40ASTM D1894
Coefficient of Friction, Static 0.500.50ASTM D1894
Film Tensile Strength at Break, MD 215 MPa31200 psiASTM D882A
Film Tensile Strength at Break, TD 290 MPa42100 psiASTM D882A
 
Optical PropertiesMetricEnglishComments
Haze 3.6 %3.6 %Gardner; ASTM D1003
Transmission, Visible 88.5 %88.5 %ASTM D1003
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Intercontinental Polymers 1128 Bicomponent PBT/PET Fiber Type - 1.8 Denier X 3 Inches
Overview of materials for Stainless Steel
GEHR Plastics ECO-GEHR® PA CL Cellulose-Lignin Compound
FKuR Kunststoff Bio-Flex® FX 1803 Compostable PLA Blend
Elektro-Isola Etronax P EP Phenolic, Polyester Fabric Reinforcement, Light Yellow, Sheets

PDU7B0 / 33200

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.