MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.

Sandvik Nifethal 70 Resistance Wire
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: NIFETHAL 70 is an alloy with low resistivity and high temperature coefficient of resistance. Typical applications for NIFETHAL 70 are in voltage regulators, timing devices, temperature sensitive resistors, temperature compensating devices and low temperature heating applications.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.45 g/cc0.305 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 640 MPa
@Thickness 0.500 mm
92800 psi
@Thickness 0.0197 in
Tensile Strength, Yield 240 MPa
@Strain 0.2 %,
Thickness 0.500 mm
34800 psi
@Strain 0.2 %,
Thickness 0.0197 in
Elongation at Break 30 %
@Thickness 0.500 mm
30 %
@Thickness 0.0197 in
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000200 ohm-cm0.0000200 ohm-cm
 0.0000284 ohm-cm
@Temperature 100 °C
0.0000284 ohm-cm
@Temperature 212 °F
 0.0000336 ohm-cm
@Temperature 150 °C
0.0000336 ohm-cm
@Temperature 302 °F
 0.0000382 ohm-cm
@Temperature 200 °C
0.0000382 ohm-cm
@Temperature 392 °F
 0.0000438 ohm-cm
@Temperature 250 °C
0.0000438 ohm-cm
@Temperature 482 °F
 0.0000494 ohm-cm
@Temperature 300 °C
0.0000494 ohm-cm
@Temperature 572 °F
 0.0000550 ohm-cm
@Temperature 350 °C
0.0000550 ohm-cm
@Temperature 662 °F
 0.0000606 ohm-cm
@Temperature 400 °C
0.0000606 ohm-cm
@Temperature 752 °F
 0.0000668 ohm-cm
@Temperature 450 °C
0.0000668 ohm-cm
@Temperature 842 °F
 0.0000732 ohm-cm
@Temperature 500 °C
0.0000732 ohm-cm
@Temperature 932 °F
Curie Temperature 610 °C1130 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 15.0 µm/m-°C
@Temperature 20.0 - 100 °C
8.33 µin/in-°F
@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.520 J/g-°C
@Temperature 20.0 °C
0.124 BTU/lb-°F
@Temperature 68.0 °F
Thermal Conductivity 17.0 W/m-K
@Temperature 20.0 °C
118 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 1430 °C2610 °F
Maximum Service Temperature, Air 600 °C1110 °F
 
Component Elements PropertiesMetricEnglishComments
Iron, Fe 28 %28 %
Nickel, Ni 72 %72 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Special Metals Nickel 270
Sandvik Nifethal 52 Resistance Wire
Sandvik Kanthal Redi Iron 120 Resistance heating wire and resistance wire
Overview of materials for Nickel Alloy
Kanthal® 70 Resistor Material

NSANDV089 / 18983

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.