Physical Properties | Metric | English | Comments |
---|
Density | 1.14 g/cc | 0.0412 lb/in³ |
Water Absorption | 1.2 % @Time 86400 sec | 1.2 % @Time 24.0 hour |
Moisture Absorption at Equilibrium | 2.4 % | 2.4 % |
Linear Mold Shrinkage, Flow | 0.020 cm/cm @Thickness 2.00 mm | 0.020 in/in @Thickness 0.0787 in |
Linear Mold Shrinkage, Transverse | 0.020 cm/cm @Thickness 2.00 mm | 0.020 in/in @Thickness 0.0787 in |
|
Mechanical Properties | Metric | English | Comments |
---|
Tensile Strength at Break | 45.0 MPa | 6530 psi |
| 60.0 MPa | 8700 psi |
Tensile Strength, Yield | 55.0 MPa | 7980 psi |
| 88.0 MPa | 12800 psi |
Elongation at Break | 20 % | 20 % |
| >= 50 % | >= 50 % |
Elongation at Yield | 5.0 % | 5.0 % |
| 20 % | 20 % |
Tensile Modulus | 1.60 GPa | 232 ksi |
| 3.30 GPa | 479 ksi |
Flexural Strength | 30.0 MPa | 4350 psi |
| 105 MPa | 15200 psi |
Flexural Modulus | 1.05 GPa | 152 ksi |
| 3.30 GPa | 479 ksi |
Poissons Ratio | 0.40 | 0.40 |
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -30.0 °C | 2.38 ft-lb/in² @Temperature -22.0 °F |
| 6.00 kJ/m² @Temperature 23.0 °C | 2.86 ft-lb/in² @Temperature 73.4 °F |
| 7.00 kJ/m² @Temperature -30.0 °C | 3.33 ft-lb/in² @Temperature -22.0 °F |
| 23.0 kJ/m² @Temperature 23.0 °C | 10.9 ft-lb/in² @Temperature 73.4 °F |
Charpy Impact Unnotched | NB @Temperature -30.0 °C | NB @Temperature -22.0 °F |
| NB @Temperature -30.0 °C | NB @Temperature -22.0 °F |
| NB @Temperature 23.0 °C | NB @Temperature 73.4 °F |
| NB @Temperature 23.0 °C | NB @Temperature 73.4 °F |
Charpy Impact, Notched | 0.500 J/cm² @Temperature -30.0 °C | 2.38 ft-lb/in² @Temperature -22.0 °F |
| 0.600 J/cm² @Temperature 23.0 °C | 2.86 ft-lb/in² @Temperature 73.4 °F |
| 0.700 J/cm² @Temperature -30.0 °C | 3.33 ft-lb/in² @Temperature -22.0 °F |
| 2.30 J/cm² @Temperature 23.0 °C | 10.9 ft-lb/in² @Temperature 73.4 °F |
|
Electrical Properties | Metric | English | Comments |
---|
Volume Resistivity | 1.00e+13 ohm-cm @Thickness 0.750 mm | 1.00e+13 ohm-cm @Thickness 0.0295 in |
Dielectric Strength | 26.0 kV/mm @Thickness 1.00 mm | 660 kV/in @Thickness 0.0394 in |
Arc Resistance | 120 - 180 sec @Thickness 3.00 mm | 120 - 180 sec @Thickness 0.118 in |
Comparative Tracking Index | 600 V @Thickness 3.00 mm | 600 V @Thickness 0.118 in |
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 0.750 mm | 7.0 - 15 sec @Thickness 0.0295 in |
| 15 - 30 sec @Thickness 1.50 mm | 15 - 30 sec @Thickness 0.0591 in |
| 30 - 60 sec @Thickness 3.00 mm | 30 - 60 sec @Thickness 0.118 in |
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 0.750 mm | >= 120 arcs @Thickness 0.0295 in |
| >= 120 arcs @Thickness 1.50 mm | >= 120 arcs @Thickness 0.0591 in |
| >= 120 arcs @Thickness 3.00 mm | >= 120 arcs @Thickness 0.118 in |
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min |
|
Thermal Properties | Metric | English | Comments |
---|
CTE, linear, Parallel to Flow | 100 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C | 55.6 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
CTE, linear, Transverse to Flow | 100 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C | 55.6 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
Melting Point | 260 °C | 500 °F |
Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F |
Deflection Temperature at 1.8 MPa (264 psi) | 72.0 °C | 162 °F |
UL RTI, Electrical | 130 °C @Thickness 0.750 mm | 266 °F @Thickness 0.0295 in |
| 130 °C @Thickness 1.50 mm | 266 °F @Thickness 0.0591 in |
| 130 °C @Thickness 3.00 mm | 266 °F @Thickness 0.118 in |
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 0.750 mm | 167 °F @Thickness 0.0295 in |
| 75.0 °C @Thickness 1.50 mm | 167 °F @Thickness 0.0591 in |
| 75.0 °C @Thickness 3.00 mm | 167 °F @Thickness 0.118 in |
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 0.750 mm | 185 °F @Thickness 0.0295 in |
| 85.0 °C @Thickness 1.50 mm | 185 °F @Thickness 0.0591 in |
| 85.0 °C @Thickness 3.00 mm | 185 °F @Thickness 0.118 in |
Flammability, UL94 | V-2 @Thickness 0.750 mm | V-2 @Thickness 0.0295 in |
| V-2 @Thickness 1.50 mm | V-2 @Thickness 0.0591 in |
| V-2 @Thickness 3.00 mm | V-2 @Thickness 0.118 in |
Oxygen Index | 26 % | 26 % |
Glow Wire Ignition Temperature | 850 °C @Thickness 0.750 mm | 1560 °F @Thickness 0.0295 in |
| 850 °C @Thickness 1.50 mm | 1560 °F @Thickness 0.0591 in |
| 850 °C @Thickness 3.00 mm | 1560 °F @Thickness 0.118 in |
Glow Wire Flammability Index | 960 °C @Thickness 0.750 mm | 1760 °F @Thickness 0.0295 in |
| 960 °C @Thickness 1.50 mm | 1760 °F @Thickness 0.0591 in |
| 960 °C @Thickness 3.00 mm | 1760 °F @Thickness 0.118 in |
|
Processing Properties | Metric | English | Comments |
---|
Rear Barrel Temperature | 260 - 280 °C | 500 - 536 °F |
Middle Barrel Temperature | 270 - 285 °C | 518 - 545 °F |
Front Barrel Temperature | 280 - 290 °C | 536 - 554 °F |
Nozzle Temperature | 280 - 300 °C | 536 - 572 °F |
Melt Temperature | 285 - 300 °C | 545 - 572 °F |
Mold Temperature | 65.0 - 95.0 °C | 149 - 203 °F |
Drying Temperature | <= 70.0 °C @Time 3600 - 10800 sec | <= 158 °F @Time 1.00 - 3.00 hour |
|
Compliance Properties | Metric | English | Comments |
---|
European Food 1935/2004 | Yes | Yes |
FDA | Yes | Yes |
|
Descriptive Properties |
---|
Agency Ratings | ASTM D 4066 PA0111 |
| ASTM D 6779 PA0111 |
| EU 10/2011 |
| EU 2023/2006 |
| FED L-P-410A |
| MIL M-20693B |
| SAE J1639 PA0121 Z6 |
Automotive Specifications | Ford WSK-M4D647-A |
| GM GMP.PA66.005 |
Outdoor Suitability UL746C) | f2 |
Suggested Max Regrind (%) | 25 |
Uses | Cable Ties |
| Circuit Board Standoffs |
| Clamps |
| Clips |
| Connectors |
| Electrical/Electronic Applications |
| Fasteners |
| Housings |
| Industrial Applications |
| Terminal Blocks |