MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Axiall 2400F Plenum Flexible PVC  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Wire and Cable Grade

Material Notes: Plenum-grade optical fiber buffer compound. UL QMTM2 recognized component for plenum cable compound.

Information provided by Georgia Gulf

Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.59 - 1.63 g/cc1.59 - 1.63 g/ccASTM D-792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 41 - 4741 - 47delayed; ASTM D-2240
Tensile Strength, Yield 18.6 MPa2700 psiASTM D-638
Elongation at Yield 216 %216 %Air Aging: 7 days @ 113°C; 30-mil plaques; UL 1581
 270 %270 %ASTM D-638
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -9.00 °C15.8 °FASTM D-746
Oxygen Index 50 %50 %ASTM D-638
 
Processing PropertiesMetricEnglishComments
Melt Temperature 188 °C370 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Fainplast Compounds PM 7010 Flexible PVC, Extrusion
Axiall 1275 Plenum Flexible PVC
Axiall 4520 Flexible PVC
Axiall 4590 Flexible PVC
Axiall 1651 Clear 7002 Flexible PVC

PGGUL079 / 41355

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.