MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Cri-Tech LS-715 FKM Fluoroelastomer, Durometer 70A
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: The LS compounds are designed to give part shrinkage (out of the mold) and post-curing operation comparable to a nitrile or similar elastomers. In most cases, tooling changes are not required when switching over to an LS compound. NPC indicates no post-cure required to achieve high tensile and modulus values with good compression set and aging characteristics. FKHT is a high temperature resistant, low compression set compound. FKX is a high viscosity, high green strength, black fluorocarbon compound formulated for HAV and/or salt bath curing of O-ring cord and extruded profiles.

Information provided by Cri-Tech Performance Materials, an independent subsidiary of Daikin America.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.96 g/cc0.0708 lb/in³
Mooney Viscosity 70
@Temperature 121 °C
70
@Temperature 250 °F
ML1+10
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070
Tensile Strength 11.7 MPa1700 psi
Elongation at Break 300 %300 %
100% Modulus 4.41 MPa
@Strain 100 %
640 psi
@Strain 100 %
Compression Set 21 %
@Temperature 200 °C,
Time 79200 sec
21 %
@Temperature 392 °F,
Time 22.0 hour
Plied disc

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
KKPC KOSYN 1507H Styrene Butadiene Rubber
KKPC KOSYN 1500 Styrene Butadiene Rubber
Sibur SKS-30 ARKPN 1st Group Styrene-Butadiene Rubber (SBR)
Trelleborg Z800 Commercial SBR Rubber
Dynasol Calprene® 1015 Styrene-Butadiene Rubber SBR Diblock Copolymer

PDAIK966 / 210219

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.