MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SSAB Tunnplat Docol® 260 BH High-strength Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel

Material Notes: High-strength Steel

Comments: Docol BH - Cold Rolled Steel - rephosphorized steel with bake hardening effect. Property values are for cold-rolled steel; thicknesses 0.40 - 2.0 mm. Iron content is approximate - exact composition is not reported by the manufacturer.

Data provided by SSAB Tunnplat.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.87 g/cc0.284 lb/in³Estimated by MatWeb
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 380 - 460 MPa55100 - 66700 psi
Tensile Strength, Yield  260 - 320 MPa
@Strain 0.2 %
37700 - 46400 psi
@Strain 0.2 %
 >= 310 MPa
@Strain 2 %
>= 45000 psi
@Strain 2 %
bake hardening after 2% strain and heating to 170°C for 20 min.
Elongation at Break >= 28 %>= 28 %A80
 
Component Elements PropertiesMetricEnglishComments
Iron, Fe 98 %98 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SSAB Tunnplat Docol® DC06 (Fe P06) Deep-drawing Steel
ArcelorMittal 260 BH Bake hardening steel, Cold rolled
Cymat A35620SC 020SS Stabilized Aluminum Foam
ArcelorMittal FF 280 D Very High Strength Cold Rolled Steel
Molybdenum, Mo, Annealed

NTUNN36 / 19528

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.