MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Vycom FLAMETEC™ CPVC Chlorinated Polyvinyl Chloride Sheet
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Flametec™ CPVC made from Corzan® 4910 white 120 compound is a high heat, corrosion resistant chlorinated polyvinyl chloride sheet. Because of its excellent corrosion resistance at elevated temperatures, it is ideally suited for self-supporting constructions where high temperatures are a concern. It can be used (depending on chemistry) up to 212°F. The Corzan® 4910 compound was especially designed to meet FM 4910 Clean Room Protocol and it is considered to be a non-fire-propagating material. Flametec CPVC sheet made from Corzan® 4910 compound is listed in accordance with the FMRC 4910 protocol and it has a class 1 rating in accordance to UL 2360e.

FEATURES AND BENEFITS

  • Chemical Resistance- Stability after exposure to semiconductor process chemistry.
  • Strength- Structural integrity to design process tools.
  • Weldability- Flametec™ CPVC can be easily fabricated using conventional hot air and automated welding equipment.
  • Fire Safe- Flametec™ CPVC compound is listed in accordance to FM 4910 protocol and has a class 1 rating in accordance to UL 2360.

Information provided by Compression Polymers Corp - Vycom

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.55 g/cc0.0560 lb/in³ASTM D792
Water Absorption 0.030 %0.030 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 119119ASTM D785
Tensile Strength, Ultimate 54.5 MPa7900 psiASTM D638
Flexural Strength 100 MPa14500 psiASTM D790
Flexural Modulus 3.15 GPa457 ksiASTM D790
Compressive Strength 69.6 MPa10100 psiASTM D695
Compressive Modulus 1.35 GPa196 ksiASTM D695
Izod Impact, Notched 0.801 J/cm1.50 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.40e+15 ohm-cm3.40e+15 ohm-cmASTM D257
Dielectric Constant 3.7
@Frequency 60 Hz
3.7
@Frequency 60 Hz
ASTM D150
Dielectric Strength 49.2 kV/mm1250 kV/inASTM D147
Dissipation Factor 0.000070
@Frequency 60 Hz
0.000070
@Frequency 60 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 66.6 µm/m-°C
@Temperature 20.0 °C
37.0 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.140 W/m-K0.972 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 1.8 MPa (264 psi) 103 °C217 °FASTM D648
Flammability, UL94 5VB
@Thickness 1.57 mm
5VB
@Thickness 0.0620 in
Oxygen Index 60 %60 %ASTM D2863
 
Descriptive Properties
Factory Mutual4910 ListedFile #3002299

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Vycom Corzan® CPVC Chlorinated PVC
Overview of materials for Chlorinated PVC (CPVC)
GEHR Plastics PVC-C®
Axiall ProTherm® 4526 CPVC Rigid PVC, Molding
Geon® Performance Solutions CPVC LC500 Polyvinyl Chloride, Chlorinated (CPVC)

PCPCV05 / 29077

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.