Product Description: Enable 20-05 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and puncture. Easier processing and excellent properties lead to significant high pressure LDPE replacement in many applications, yet with superior drawdown and enhanced toughness. Enable 20-05 resins are available for blown film both formulated and non-formulated. Availability: Asia Pacific Additive: - Antiblock: 2000 ppm
- Slip: 500 ppm
- Processing Aid: Yes
- Thermal Stabilizer: Yes
Applications:- Agricultural Film
- Blown Film
- Cast Film
- Cast Stretch Film
- Collation Shrink
- Food packaging
- Form Fill and Seal Packaging
- Heavy Duty Bags
- Lamination Film
- Multilayer Packaging Film
- Shrink Film
- Stand Up Pouches
- Stretch Film
Information provided by ExxonMobil |