MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PTS Trilac® ABS-HH2350 High Heat ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded

Material Notes: Information provided by Polymer Technology and Services, LLC (PTS).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ASTM D792
Melt Flow 4.5 g/10 min
@Load 10.0 kg,
Temperature 220 °C
4.5 g/10 min
@Load 22.0 lb,
Temperature 428 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 112112ASTM D785
Tensile Strength, Yield 48.9 MPa7090 psiASTM D638
Flexural Yield Strength 70.4 MPa10200 psiASTM D790
Flexural Modulus 2.34 GPa339 ksiASTM D790
Izod Impact, Notched 1.28 J/cm
@Thickness 3.17 mm
2.40 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 114 °C237 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 104 °C219 °FASTM D648
Flammability, UL94 HB
@Thickness 6.35 mm
HB
@Thickness 0.250 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aclo Accuguard ABS ABS860V0L Flame Retardant
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled
Wacker Geniomer® 60 Silicone TPE
Covestro Bayblend® T65 XF Polycarbonate + ABS

PZ9PT05 / 21468

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.