MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® A 218 V40 Black 21 NHFE PA66, 40% glass fiber, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled

Material Notes: Description: Polyamide 66, offering high flowability and productivity gains, reinforced with 40% of glass fiber, heat stabilized, for injection molding.

Available in: Europe

Product Applications: TECHNYL ® A 218 V40 BLACK 21NHFE is characterized by a high flowability and offers an excellent combination between thermal and mechanical properties. This grade is ideal for use in the automotive industry for engine components, such as: inlet manifolds, air ducts - engine covers, and various housings and liquid containers. This product is available in black.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.46 g/cc0.0527 lb/in³ISO 1183/A
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 155 MPa22500 psiISO 527 Type 1A
Elongation at Break 3.5 %3.5 %ISO 527 Type 1A
Tensile Modulus 9.60 GPa1390 ksiISO 527 Type 1A
Flexural Strength 230 MPa33400 psiISO 178
Flexural Modulus 7.60 GPa1100 ksiISO 178
Izod Impact, Notched (ISO) 18.0 kJ/m²8.57 ft-lb/in²ISO 180/1eA
Charpy Impact Unnotched 9.80 J/cm²46.6 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.90 J/cm²9.04 ft-lb/in²ISO 179/1eA
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.20 %<= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TECHNYL® A 218 V40 PA66, 40% glass fiber, DRY
Domo TECHNYL® A 218 V40 PA66, 40% glass fiber, Conditioned
Domo Technyl® A 216 V40 40% Glass Filled Nylon 66
Domo TECHNYL® C 216 V40 PA6, 40% glass fiber, DRY
Domo TECHNYL® C 216 V40 PA6, 40% glass fiber, Conditioned

PRHOD648 / 137879

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.