MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® 8270 HS PA6 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Ultramid 8270 HS is a thermally modified PA6 blow molding compound exhibiting exceptional toughness and melt strength ideally suited for blow molding, profile extrusion, and other applications requiring extra high melt viscosity. It exhibits excellent permeability and chemical resistance to oils, hydrocarbons and most solvents.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ISO 1183
Water Absorption 1.6 %1.6 %24 hour; ISO Test
 9.2 %9.2 %ISO 62
Moisture Absorption at Equilibrium 2.6 %2.6 %23°C/50% R.H.; ISO 62
Viscosity Measurement 220220Formic Acid
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9999ASTM Test
Tensile Strength, Yield 84.0 MPa12200 psi50mm/min; ISO 527
 84.0 MPa12200 psi2 in/min; ASTM Test
 24.0 MPa
@Temperature 120 °C
3480 psi
@Temperature 248 °F
ISO Data
 24.0 MPa
@Temperature 120 °C
3480 psi
@Temperature 248 °F
ASTM Test
 138 MPa
@Temperature -40.0 °C
20000 psi
@Temperature -40.0 °F
ASTM Test
 138 MPa
@Temperature -40.0 °C
20000 psi
@Temperature -40.0 °F
ISO Data
Elongation at Break >= 100 %>= 100 %2 in/min; ASTM Test
Elongation at Yield 4.0 %4.0 %50mm/min; ISO 527
 4.0 %4.0 %2 in/min; ASTM Test
Flexural Strength 114 MPa16500 psiASTM Test
 17.0 MPa
@Temperature 120 °C
2470 psi
@Temperature 248 °F
ASTM Test
 20.0 MPa
@Temperature 93.0 °C
2900 psi
@Temperature 199 °F
ASTM Test
 30.0 MPa
@Temperature 65.0 °C
4350 psi
@Temperature 149 °F
ASTM Test
 179 MPa
@Temperature -40.0 °C
26000 psi
@Temperature -40.0 °F
ASTM Test
Flexural Modulus 0.310 GPa45.0 ksi
 2.90 GPa421 ksiASTM Test
 0.260 GPa
@Temperature 120 °C
37.7 ksi
@Temperature 248 °F
ASTM Test
 0.435 GPa
@Temperature 65.0 °C
63.1 ksi
@Temperature 149 °F
ASTM Test
Izod Impact, Notched 0.530 J/cm
@Temperature -40.0 °C
0.993 ft-lb/in
@Temperature -40.0 °F
ASTM Test
 0.530 J/cm
@Thickness 3.17 mm
0.993 ft-lb/in
@Thickness 0.125 in
ASTM Test
 
Thermal PropertiesMetricEnglishComments
CTE, linear 135 µm/m-°C
@Temperature -30.0 - 30.0 °C
75.0 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM Test
Melting Point 220 °C428 °F10 K/min
 220 °C428 °FASTM Test
Deflection Temperature at 0.46 MPa (66 psi) 169 °C336 °FASTM Test
Deflection Temperature at 1.8 MPa (264 psi) 63.0 °C145 °FASTM Test
Flammability, UL94 HBHB
 HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
 
Descriptive Properties
ColorNatural
Commercial StatusActive America
FormPellets
Impact ModifiedNo
Primary Processing TechniqueBlow Molding
ProcessingBlow molding
 Injection Molding
Special characteristicHeat stabilized or stable to heat
UL.UL-CYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® 8270 HS BK 102 PA6 (Dry)
BASF Ultramid® 8350 HS PA6 (Dry)
Envalior Akulon® F136-E2 PA6
BASF Ultramid® 8270 HS PA6 (Conditioned)
BASF Ultramid® 8270 HS BK 102 PA6 (Conditioned)

PBASF9197 / 84961

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.