MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aluminum Bronze, 5%, UNS C60600, H04 Temper
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Good to excellent corrosion resistance. Good lubrication and cooling essential for good finish.Applications: Produced as sheet, strip, rolled bar; used to make fasteners, deep drawn "gold" decoration, and parts requiring corrosion resistance.

Inactive per the Copper Development Association.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.17 g/cc0.295 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 5555
Tensile Strength, Ultimate 415 MPa
@Thickness 13.0 mm
60200 psi
@Thickness 0.512 in
plate
Tensile Strength, Yield 165 MPa
@Thickness 13.0 mm
23900 psi
@Thickness 0.512 in
plate
Elongation at Break 25 %
@Thickness 13.0 mm
25 %
@Thickness 0.512 in
In 50 mm, plate
Modulus of Elasticity 121 GPa17500 ksi
Poissons Ratio 0.3260.326
Machinability 20 %20 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 46.0 GPa6670 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000100 ohm-cm
@Temperature 20.0 °C
0.0000100 ohm-cm
@Temperature 68.0 °F
Magnetic Permeability 1.011.01
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 - 300 °C
10.0 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.375 J/g-°C0.0896 BTU/lb-°F
Thermal Conductivity 79.5 W/m-K552 BTU-in/hr-ft²-°F
Melting Point 1050 - 1065 °C1920 - 1949 °F
Solidus 1050 °C1920 °F
Liquidus 1065 °C1949 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 550 - 650 °C1020 - 1200 °F
Hot-Working Temperature 815 - 870 °C1500 - 1600 °F
Recrystallization Temperature 350 °C662 °F44% reduction and 0.075 mm initial grain size
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 4.0 - 7.0 %4.0 - 7.0 %
Copper, Cu 92 - 96 %92 - 96 %
Iron, Fe <= 0.50 %<= 0.50 %
Other, total <= 0.50 %<= 0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum Bronze, UNS C61300, Annealed
Aluminum Bronze, UNS C61300, O60 Temper
Aluminum Bronze, 5%, UNS C60600, O60 Temper
Nickel Aluminum Bronze, UNS C63000, HR50 Temper
Aluminum Bronze D, UNS C61400, H04 Temper 25 mm flat products

MC60600b2 / 11575

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.