MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Grade 704 Zirconium (Zr-1.5Sn)
Categories: Metal; Nonferrous Metal; Zirconium Alloy

Material Notes: Characteristics:
  • Contains halfnium
  • Mechanical Properties similar to pure zirconium, stronger and less ductile
  • Excellent corrosion resistance
  • Forms a stable, dense, self-healing oxide layer
  • Highly anisotropic

Applications: Chemical processing equipment

Machining Parameters: Use slow speeds, heavy feeds and flood cooling with a water-soluble oil lubricant.

Key Words: UNS R60704, Zircadyne® 704
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 6.56 g/cc0.237 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate >= 413 MPa>= 59900 psi
 220 MPa
@Temperature 400 °C
31900 psi
@Temperature 752 °F
 260 MPa
@Temperature 300 °C
37700 psi
@Temperature 572 °F
 360 MPa
@Temperature 200 °C
52200 psi
@Temperature 392 °F
 480 MPa
@Temperature 100 °C
69600 psi
@Temperature 212 °F
 530 MPa
@Temperature 20.0 °C
76900 psi
@Temperature 68.0 °F
Tensile Strength, Yield  120 MPa
@Temperature 400 °C
17400 psi
@Temperature 752 °F
 140 MPa
@Temperature 300 °C
20300 psi
@Temperature 572 °F
 190 MPa
@Temperature 200 °C
27600 psi
@Temperature 392 °F
 280 MPa
@Temperature 100 °C
40600 psi
@Temperature 212 °F
 360 MPa
@Temperature 20.0 °C
52200 psi
@Temperature 68.0 °F
 >= 241 MPa
@Strain 0.2 %
>= 35000 psi
@Strain 0.2 %
Elongation at Break 14 %14 %in 50 mm
 22 %
@Temperature 20.0 °C
22 %
@Temperature 68.0 °F
 26 %
@Temperature 100 °C
26 %
@Temperature 212 °F
 32 %
@Temperature 200 °C
32 %
@Temperature 392 °F
 34 %
@Temperature 400 °C
34 %
@Temperature 752 °F
 38 %
@Temperature 310 °C
38 %
@Temperature 590 °F
Modulus of Elasticity 99.3 GPa14400 ksi
Poissons Ratio 0.370.37
Shear Modulus 36.2 GPa5250 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000740 ohm-cm0.0000740 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 6.00 µm/m-°C
@Temperature 25.0 °C
3.33 µin/in-°F
@Temperature 77.0 °F
Specific Heat Capacity 0.285 J/g-°C0.0681 BTU/lb-°F
Thermal Conductivity 21.5 W/m-K149 BTU-in/hr-ft²-°F
Melting Point 1850 °C3360 °F
Boiling Point 4375 °C7907 °F
 
Component Elements PropertiesMetricEnglishComments
Fe + Cr 0.30 %0.30 %
Hafnium, Hf <= 4.5 %<= 4.5 %
Oxygen, O 0.18 %0.18 %
Tin, Sn 1.5 %1.5 %
Zirconium, Zr >= 97.5 %>= 97.5 %includes Hf
 
Descriptive Properties
Alpha Phase Crystal Structurehcp< 865°C
Beta Phase Crystal Structurebcc> 865°C

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zirconium Oxide, Zirconia, ZrO2
Zircaloy-2 Zirconium Alloy
Zircaloy-4 Zirconium Alloy
Grade 702 Zirconium, Commercially Pure
Assab Steels 8407 SUPREME Hot Work Steel

MZRI10 / 14571

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.