MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik Vestamid® L2141 Black Nylon 12  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Description: High-viscosity, higher heat stability than L2140, light-stabilized, with processing aid

Applications: Tubing for hydraulic clutches, vacuum lines

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Key Words: PA12, EHL,22-010
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.70 %
@Thickness 1.00 mm,
Temperature 23.0 °C
0.70 %
@Thickness 0.0394 in,
Temperature 73.4 °F
50% R.H.; ISO 62
Water Absorption at Saturation 1.5 %
@Thickness 1.00 mm
1.5 %
@Thickness 0.0394 in
ISO 62
Linear Mold Shrinkage 0.012 cm/cm0.012 in/in127x12.7x3.2 mm (processing cond. acc. To ISO 1874-2)
Linear Mold Shrinkage, Transverse 0.014 cm/cm0.014 in/in127x12.7x3.2 mm (processing cond. acc. To ISO 1874-2)
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 46.0 MPa6670 psiISO 527-1/2
Elongation at Break >= 50 %>= 50 %ISO 527-1/2
Elongation at Yield 5.0 %5.0 %ISO 527-1/2
Tensile Modulus 1.50 GPa218 ksiISO 527-1/2
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.800 J/cm²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmIEC 60093
Dielectric Constant  4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
IEC 60250
 9.7
@Frequency 100 Hz
9.7
@Frequency 100 Hz
IEC 60250
Dielectric Strength 35.0 kV/mm889 kV/inK20/P50; IEC 60243-1
Dissipation Factor  0.11
@Frequency 1e+6 Hz
0.11
@Frequency 1e+6 Hz
IEC 60250
 0.21
@Frequency 100 Hz
0.21
@Frequency 100 Hz
IEC 60250
Comparative Tracking Index >= 600 V>= 600 VTest Solution A, 50 drops; IEC 60112
 600 V600 VTest Solution A, 100 drops; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 150 µm/m-°C
@Temperature 23.0 - 55.0 °C
83.3 µin/in-°F
@Temperature 73.4 - 131 °F
45x15x10 mm; ISO 11359
Melting Point 178 °C352 °FPeak Temperature; ISO 3146, ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 110 °C230 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °FISO 75
Vicat Softening Point 140 °C284 °F50N; ISO 306
 170 °C338 °F10N; ISO 306
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
 
Descriptive Properties
Electrolytic CorrosionA1 StepIEC 60426

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik VESTAMID® DX9304 PA 612 Dry
Arkema Rilsamid® AECHVO TL PA12
Arkema Rilsamid® AESN BLACK P202 T6L PA12-I
Evonik VESTAMID® EX9200 PA 12
EMS-Grivory Grilamid® L 20 HL black 9563 PA12

PHULA39 / 47399

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.