MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nitrogen, N2
Categories: Fluid; Pure Element

Key Words: Nitrogen, N2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.001145 g/cc0.00004137 lb/in³Gas
Molecular Weight 28.013 g/mol28.013 g/mol
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 14.006714.00671995
Atomic Number 77
X-ray Absorption Edge 30.99 Å30.99 ÅK
Critical Pressure 33.9000 bar25427.1 torr
Critical Temperature -146.94 °C-232.49 °F
Critical Molar Volume 90.0 cm³/mol5.49 in³/mol
Electronegativity 3.043.04Pauling
Ionic Radius 0.130 Å0.130 ÅCrystal Ionic Radius for Valence +5
 0.160 Å0.160 ÅCrystal Ionic Radius for Valence +3
 0.250 Å0.250 ÅCrystal Ionic Radius for Valence +1
 1.71 Å1.71 ÅCrystal Ionic Radius for Valence -3
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 25.35 J/g10.90 BTU/lb
Heat of Vaporization 198.8 J/g85.54 BTU/lbAt Boiling Point
Specific Heat Capacity 1.039 J/g-°C0.2483 BTU/lb-°F
Thermal Conductivity  0.00980 W/m-K
@Pressure 0.100 MPa,
Temperature -173 °C
0.0680 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature -280 °F
gas
 0.0187 W/m-K
@Pressure 0.100 MPa,
Temperature -73.1 °C
0.130 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature -99.7 °F
gas
 0.0260 W/m-K
@Pressure 0.100 MPa,
Temperature 26.9 °C
0.180 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 80.3 °F
gas
 0.0323 W/m-K
@Pressure 0.100 MPa,
Temperature 127 °C
0.224 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 260 °F
gas
 0.0383 W/m-K
@Pressure 0.100 MPa,
Temperature 227 °C
0.266 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 440 °F
gas
 0.0440 W/m-K
@Pressure 0.100 MPa,
Temperature 327 °C
0.305 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 620 °F
gas
Melting Point -210 °C-346 °F
Boiling Point -195.79 °C-320.42 °F
Heat of Formation 0.000 kJ/mol0.000 kJ/molGas
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.19876
@Temperature -196 °C,
Wavelength 578 nm
1.19876
@Temperature -321 °F,
Wavelength 578 nm
 
Component Elements PropertiesMetricEnglishComments
Nitrogen, N 100 %100 %
 
Descriptive Properties
AppearanceColorless Gas
CAS Number7727-37-9

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hydrogen, H2
Argon, Ar
Oxygen (O2)
Graphite, Carbon, C
Helium, He

AMEN / 64

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.