MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Nypel® 2314 HS BK6 PA6 (Dry)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Description: Nypel® 2314 HS BK6 is a black pigmented, low viscosity, heat stabilized, semi crystalline, injection molding compound based on recycled PA6 feedstocks. It also offers the following: good chemical and thermal aging resistance, good flow and processability, as well as good dimensional stability.

Application: Nypel® 2314 HS BK6 is generally recommended for applications such as hardware, handles, clips and fasteners.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ISO 1183
Moisture Absorption at Equilibrium 1.6 %1.6 %24 Hours
 2.7 %2.7 %50% RH
 9.5 %9.5 %Saturation
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 80.0 MPa11600 psiISO 527
Elongation at Break 44 %44 %Nominal; ISO 527
Flexural Modulus 2.62 GPa380 ksiISO 178
Izod Impact, Notched (ISO) 5.50 kJ/m²2.62 ft-lb/in²ISO 180
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 58.0 °C136 °FISO 75
UL RTI, Electrical 65.0 °C
@Thickness 1.50 mm
149 °F
@Thickness 0.0591 in
746B
UL RTI, Mechanical with Impact 65.0 °C
@Thickness 1.50 mm
149 °F
@Thickness 0.0591 in
746B
UL RTI, Mechanical without Impact 65.0 °C
@Thickness 1.50 mm
149 °F
@Thickness 0.0591 in
746B
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 - 285 °C464 - 545 °F
Mold Temperature 65.0 - 80.0 °C149 - 176 °F
Dry Time 2 - 4 hour2 - 4 hour
Moisture Content 0.15 %0.15 %
 
Descriptive Properties
ColorBK 6
Commercial StatusNorth America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® B3K PA6 (Conditioned)
BASF Ultramid® B3K PA6 (Dry)
BASF Nypel® 2351 HS BK PA6 (Dry)
Cast Nylons Nycast® 6MPB Plasticized Nylon 6
Celanese Zytel® 101L NC010 PA66

PBASG0547 / 132180

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.