MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Exxtra™ Seal m 1012.MK Metallocene Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Product Description: Exxtra™ Seal m 1012 resins are an ethylene 1-hexene copolymers. Films made from these resins have outstanding cold temperature toughness impact strength and puncture. These superior strength properties, along with excellent heat sealing and hot tack performance, make this a very versatile packaging film resin. TnPP is not intentionally added to Exxtra™ Seal m 1012 resins

Availability: Latin America, North America and South America

Additive:

  • Antiblock: 5000 ppm
  • Slip: 1000 ppm
  • Processing Aid: Yes
  • Thermal Stabilizer: Yes
Applications:
  • Bag in Box
  • Barrier Food Packaging
  • Blown Film
  • Food packaging
  • Form Fill and Seal Packaging
  • Freezer Film
  • Heavy Duty Bags
  • Ice Bags
  • Lamination Film
  • Multilayer Packaging Film
  • Stand Up Pouches

Information provided by ExxonMobil

Key Words: Exceed™ 1012 MK
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.912 g/cc0.0329 lb/in³ExxonMobil method
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 5000 ppm5000 ppm
Slip Level 1000 ppm1000 ppm
 
Mechanical PropertiesMetricEnglishComments
Puncture Resistance 57.8 N13.0 lb (f)
Film Tensile Strength at Yield, MD 6.89 MPa1000 psiASTM D882
Film Tensile Strength at Yield, TD 6.89 MPa1000 psiASTM D882
Film Elongation at Break, MD 460 %460 %ASTM D882
Film Elongation at Break, TD 580 %580 %ASTM D882
Puncture Energy 6.21 J4.58 ft-lbExxonMobil Method
Elmendorf Tear Strength MD 200 g200 gASTM D1922
Elmendorf Tear Strength TD 300 g300 gASTM D1922
Dart Drop Test 1100 g2.43 lbASTM D1709
Film Tensile Strength at Break, MD 60.0 MPa8700 psiASTM D882
Film Tensile Strength at Break, TD 57.2 MPa8300 psiASTM D882
1% Secant Modulus, MD 110 MPa16000 psiASTM D882
1% Secant Modulus, TD 124 MPa18000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point <= 117 °C<= 242 °FPeak Melting Point; ExxonMobil method
 
Optical PropertiesMetricEnglishComments
Haze 9.5 %9.5 %ASTM D1003
Gloss 57 %57 %45°; ASTM D2457
 
Descriptive Properties
Puncture Force10 lbfExxonMobil Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Exceed™ 1012HA Metallocene Polyethylene Resin
ExxonMobil Exxtra™ Seal m 1012.MJ Metallocene Polyethylene Resin
ExxonMobil Exceed™ 1012HJ Metallocene Polyethylene Resin
ExxonMobil Exceed™ 1018HA Metallocene Polyethylene Resin
ExxonMobil Enable™ 35-05HH Metallocene Polyethylene Resin (European Grade)

PEX99027 / 175263

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.