MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman SCHULAMID® 66 MV3FR Flame Retardant Nylon 6/6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced, Flame Retardant

Material Notes:
Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.17 g/cc1.17 g/ccASTM D792
Linear Mold Shrinkage 0.011 cm/cm
@Thickness 3.175 mm
0.011 in/in
@Thickness 0.1250 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 75.2 MPa10900 psiASTM D638
Elongation at Break 5.5 %5.5 %ASTM D638
Flexural Strength 115 MPa16700 psiASTM D790
Izod Impact, Unnotched 6.62 J/cm12.4 ft-lb/inASTM D4812
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 230 °C446 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 87.2 °C189 °FASTM D648
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 305 °C536 - 581 °F
Mold Temperature 65.6 - 93.3 °C150 - 200 °F
Drying Temperature 79.4 °C175 °F
Dry Time 2 - 4 hour2 - 4 hourPredrying

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® B3 (2500) PA 6 Dry
Addiplast Addinyl B2H G15 Flame Retardant Nylon 6, 15% Glass Bead
Aclo Accucomp Polypropylene CPO407L Copolymer
A. Schulman SCHULAMID® 66 MV3H Unreinforced Nylon 6/6
A. Schulman SCHULAMID® 66 MV3 Unreinforced Nylon 6/6

PASHU342 / 25306

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.