MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Honeywell Spectra® 900 Fiber
Categories: Other Engineering Material; Composite Fibers; Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Spectra® fiber 900 was the first commercially available extended-chain, high-strength polyethylene fiber and the first in a series of Spectra® fibers. Spectra® fiber has one of the highest strength to weight ratios of any manmade fiber. Its high tenacity makes it pound-for-pound 10 times stronger than steel, more durable than polyester and gives it a specific strength that is 40 percent greater than aramid fiber. Specific performance is dependent upon denier and filament counts. Spectra® is a registered trademark of Honeywell and was formerly a product of Allied Signal.

Key Words: FRP composites, single fiber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.970 g/cc0.0350 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 2590 MPa376000 psi
Modulus of Elasticity 117 GPa17000 ksi
 
Thermal PropertiesMetricEnglishComments
Melting Point 147 °C297 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Honeywell Spectra® 1000 Fiber
DuPont™ Kevlar® 49 Aramid Fiber
DuPont™ Kevlar® 149 Aramid Fiber, diam. 12 µm
Teijin Technora® Aramid Fiber
Toyobo Dyneema® SK60 High Strength Polyethylene Fiber

PCF006 / 27993

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.