MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Formosa Plastics Formolene® FORMAX® L71709H Film (Hexene Grade) LLDPE  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Hexene, Film Grade

Material Notes: High Strength Linear Low Density Polyethylene for Film Extrusion

Formolene FORMAX® L7 is a high strength linear low density hexene copolymer polyethylene made using a gas-phase process. Film mechanical properties are significantly improved compared to competitive super hexene LLDPE film resins. FormoleneFORMAX® L7 is formulated with slip and antiblock for use in high performance film applications offering excellent extrusion processing and outstanding impact strength and tear resistance. Films exhibit good optical properties

Formolene FORMAX® L7 meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact.

Applications: Industrial packaging, Industrial liners, Coextrusion, Can liners and Consumer trash bags

Information provided by Formosa Plastics Corporation, USA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.917 g/cc0.0331 lb/in³ASTM D1505
Thickness 25.0 microns0.984 mil
Melt Flow 0.90 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.90 g/10 min
@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 11.41 MPa1655 psiASTM D882
Film Tensile Strength at Yield, TD 11.27 MPa1635 psiASTM D882
Film Elongation at Break, MD 700 %700 %ASTM D882
Film Elongation at Break, TD 870 %870 %ASTM D882
Elmendorf Tear Strength MD 375 g375 gASTM D1922
Elmendorf Tear Strength TD 705 g705 gASTM D1922
Dart Drop Test 405 g0.893 lbASTM D1709
Film Tensile Strength at Break, MD 39.2 MPa5680 psiASTM D882
Film Tensile Strength at Break, TD 29.6 MPa4290 psiASTM D882
 
Processing PropertiesMetricEnglishComments
Blow-up Ratio (BUR) 2.52.5
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total Lotrene® Q2018H Linear Low Density Polyethylene, Blown Film
Total Lotrene® Q1018H Linear Low Density Polyethylene, Blown Film
Total LLDPE LL 1820 Linear Low Density Polyethylene - Blown Film
SIDPEC EGYPTENE® LL 0205 AF LLDPE Film
Petroquimica Triunfo Trithene® TS 4016 LDPE and LLDPE Blend - Film

PFPCPQ068 / 150300

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.