MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DSM Biomedical Calo-MER™ 35 Shape Memory Thermoplastic  (discontinued **)
Categories: Polymer; Thermoplastic

Material Notes: Many implantable biomedical devices could benefit from a polymer with a strongly temperature-dependent modulus. For example, catheters made from such a polymer could be inserted as a stiff plastic and, upon reaching body temperature, would soften dramatically to minimize erosion of adjacent tissue. Calo•MER™ shape-memory thermoplastics are a family of materials that have a distinct, adjustable thermal transition that produces a dramatic change in modulus (and several other properties) over a narrow but controllable range of temperatures. Calo•MER thermoplastics can be produced with any transition temperature between -40 and 70°C, to a tolerance of ±2°C. The extent of modulus change at the transition temperature can also be easily tailored to the particular application.

Calo•MER has many potential applications in medical, industrial, and consumer products. Medical devices for which Calo•MER has been suggested include catheters, bone casts, introducers, stents, and endotracheal tubes. Industrial applications for Calo•MER include spacesuits, connectors, thermal overload devices, and temperature indicators. There is also a potential niche in the toy and novelty market for Calo•MER, where action figures, vehicles, jewelry, flowers, and building systems could benefit from its unique properties.

Calo•MER™ shape-memory thermoplastics can be melt fabricated by conventional extrusion, injection molding, or compression molding techniques. These materials are heat-sealable, readily blended with fillers, and easily post-formed.

Information provided by the manufacturer, Polymer Technology Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Flexural Modulus 0.641 GPa93.0 ksiDry
 0.00827 GPa
@Temperature 37.0 °C
1.20 ksi
@Temperature 98.6 °F
Hydrated
 0.0200 GPa
@Temperature 37.0 °C
2.90 ksi
@Temperature 98.6 °F
Dry
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 34.0 °C93.2 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DSM Biomedical CarboSil® 10 90A Biocompatible Silicone Polycarbonate Urethane
SpinTech Veritex™ Shape Memory Polymer Composite
DSM Biomedical CarboSil® 40 90A Biocompatible Silicone Polycarbonate Urethane
DSM Biomedical Calo-MER™ 40 Shape Memory Thermoplastic
DSM Biomedical Calo-MER™ 45 Shape Memory Thermoplastic

PBIOCA0 / 27168

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.