MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Polypropylene with Carbon Black Filler
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with Carbon Black Filler

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.947 - 1.43 g/cc0.0342 - 0.0517 lb/in³Average value: 1.04 g/cc Grade Count:34
Water Absorption 0.0100 - 0.200 %0.0100 - 0.200 %Average value: 0.0550 % Grade Count:8
Thickness 102 microns4.00 milAverage value: 102 microns Grade Count:8
Linear Mold Shrinkage 0.00600 - 0.0200 cm/cm0.00600 - 0.0200 in/inAverage value: 0.0132 cm/cm Grade Count:18
Melt Flow 0.100 - 35.0 g/10 min0.100 - 35.0 g/10 minAverage value: 6.57 g/10 min Grade Count:19
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 96.0 - 99.096.0 - 99.0Average value: 97.5 Grade Count:8
Hardness, Shore D 70.0 - 74.070.0 - 74.0Average value: 72.3 Grade Count:8
Tensile Strength, Ultimate 16.5 - 58.6 MPa2390 - 8500 psiAverage value: 26.9 MPa Grade Count:26
Tensile Strength, Yield 21.0 - 44.8 MPa3050 - 6500 psiAverage value: 26.7 MPa Grade Count:8
Film Elongation at Break, MD 4.00 - 500 %4.00 - 500 %Average value: 252 % Grade Count:4
Elongation at Break 2.00 - 150 %2.00 - 150 %Average value: 20.3 % Grade Count:29
Elongation at Yield 7.00 - 12.0 %7.00 - 12.0 %Average value: 9.28 % Grade Count:5
Modulus of Elasticity 0.483 - 5.52 GPa70.1 - 800 ksiAverage value: 1.80 GPa Grade Count:10
Flexural Yield Strength 0.193 - 63.8 MPa28.0 - 9250 psiAverage value: 35.6 MPa Grade Count:16
Flexural Modulus 0.951 - 5.52 GPa138 - 800 ksiAverage value: 1.92 GPa Grade Count:32
Izod Impact, Notched 0.196 - 981 J/cm0.367 - 1840 ft-lb/inAverage value: 2.28 J/cm Grade Count:21
 0.588399 - 0.588399 J/cm
@Temperature -20.0 - -20.0 °C
1.10231 - 1.10231 ft-lb/in
@Temperature -4.00 - -4.00 °F
Average value: 0.588 J/cm Grade Count:1
Izod Impact, Unnotched 1.00 J/cm - NB1.87 ft-lb/in - NBAverage value: 7.43 J/cm Grade Count:7
Izod Impact, Notched (ISO) 1.50 kJ/m² - NB0.714 ft-lb/in² - NBAverage value: 27.7 kJ/m² Grade Count:10
 1.20 kJ/m² - NB
@Temperature -20.0 - -20.0 °C
0.571 ft-lb/in² - NB
@Temperature -4.00 - -4.00 °F
Average value: 5.84 kJ/m² Grade Count:7
 1.20 kJ/m² - NB
@Thickness 4.00 - 4.00 mm
0.571 ft-lb/in² - NB
@Thickness 0.157 - 0.157 in
Average value: 5.84 kJ/m² Grade Count:7
Izod Impact, Unnotched (ISO) 16.0 kJ/m² - NB7.61 ft-lb/in² - NBAverage value: 48.7 kJ/m² Grade Count:10
 9.00 kJ/m² - NB
@Temperature -20.0 - -20.0 °C
4.28 ft-lb/in² - NB
@Temperature -4.00 - -4.00 °F
Average value: 17.7 kJ/m² Grade Count:7
 9.00 kJ/m² - NB
@Thickness 4.00 - 4.00 mm
4.28 ft-lb/in² - NB
@Thickness 0.157 - 0.157 in
Average value: 17.7 kJ/m² Grade Count:7
Charpy Impact Unnotched 1.40 - 1000 J/cm²6.66 - 4760 ft-lb/in²Average value: 1.40 J/cm² Grade Count:8
 0.500 - 999.9 J/cm²
@Temperature -20.0 - -20.0 °C
2.38 - 4759 ft-lb/in²
@Temperature -4.00 - -4.00 °F
Average value: 0.500 J/cm² Grade Count:7
 0.500 - 999.9 J/cm²
@Thickness 102 - 102 mm
2.38 - 4759 ft-lb/in²
@Thickness 4.00 - 4.00 in
Average value: 0.500 J/cm² Grade Count:7
Charpy Impact, Notched 0.300 - 5.00 J/cm²1.43 - 23.8 ft-lb/in²Average value: 2.44 J/cm² Grade Count:8
 0.200 - 2.60 J/cm²
@Temperature -20.0 - -20.0 °C
0.952 - 12.4 ft-lb/in²
@Temperature -4.00 - -4.00 °F
Average value: 1.39 J/cm² Grade Count:7
 0.200 - 2.60 J/cm²
@Thickness 102 - 102 mm
0.952 - 12.4 ft-lb/in²
@Thickness 4.00 - 4.00 in
Average value: 1.39 J/cm² Grade Count:7
Film Tensile Strength at Break, MD 25.0 - 33.0 MPa3630 - 4790 psiAverage value: 28.3 MPa Grade Count:4
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 5.00 - 1.00e+9 ohm-cm5.00 - 1.00e+9 ohm-cmAverage value: 4.84e+7 ohm-cm Grade Count:22
Surface Resistance 10.0 - 1.00e+9 ohm10.0 - 1.00e+9 ohmAverage value: 4.25e+7 ohm Grade Count:30
Static Decay 0.100 sec0.100 secAverage value: 0.100 sec Grade Count:3
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 107 - 300 °C225 - 572 °FAverage value: 185 °C Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 62.2 - 160 °C144 - 320 °FAverage value: 103 °C Grade Count:23
Deflection Temperature at 1.8 MPa (264 psi) 45.0 - 82.0 °C113 - 180 °FAverage value: 57.8 °C Grade Count:20
Vicat Softening Point 80.0 - 156 °C176 - 313 °FAverage value: 134 °C Grade Count:8
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 190 - 230 °C374 - 446 °FAverage value: 214 °C Grade Count:9
Melt Temperature 190 - 270 °C374 - 518 °FAverage value: 223 °C Grade Count:20
Mold Temperature 30.0 - 80.0 °C86.0 - 176 °FAverage value: 53.9 °C Grade Count:16
Roll Temperature 60.0 - 100 °C140 - 212 °FAverage value: 80.7 °C Grade Count:5
Drying Temperature 60.0 - 120 °C140 - 248 °FAverage value: 95.0 °C Grade Count:19
Injection Pressure 60.0 - 80.0 MPa8700 - 11600 psiAverage value: 70.0 MPa Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene, Carbon Fiber Filled
Overview of materials for Polypropylene with 30% Glass Fiber Filler
Overview of materials for Polypropylene with 10% Glass Fiber Filler
Overview of materials for Polypropylene with 20% Glass Fiber Filler
Overview of materials for Polypropylene with 60% Glass Fiber Filler

O4729 / 78387

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.