MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Sibur Neva Polyvinyl Chloride (PVC)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Molded

Material Notes: Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a period of 20 minutes. For molding of non-detachable plugs, connecting cords of electric machines and devices and for sheath of electric domestic cords. Characteristic peculiarity of plastic "Neva" is absence of sticking, changing of color of plastic during contact with metal surfaces, heated up to 150°C during 8-10 minutes.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.32 g/cc0.0477 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 17.0 MPa>= 2470 psi
Elongation at Break >= 250 %>= 250 %
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 5.00e+12 ohm-cm
@Temperature 70.0 °C
>= 5.00e+12 ohm-cm
@Temperature 158 °F
Dielectric Strength >= 20.0 kV/mm>= 508 kV/in
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -35.0 °C<= -31.0 °F
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sibur 140-13P Polyvinyl Chloride (PVC)
Overview of materials for Polyvinyl Dichloride (PVDC)
Overview of materials for PVC, Molded
Overview of materials for PVC, Extruded
Overview of materials for Polyvinyl Dichloride (PVDC) Coated Polyester Film

PSIB056 / 67619

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.