MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik BREAK-THRU® Vibrant Surfactants
Categories: Fluid

Material Notes: BREAK-THRU® Vibrant is a non-ionic organic surfactant.

Application: BREAK-THRU Vibrant can be used as a tank mix adjuvant as well as an additive for in-can formulations. BREAK-THRU Vibrant imparts a very low dynamic surface tension and improves the adhesion of pesticidal sprays. In field trials, BREAK-THRU® Vibrant has proven safe for use on crops, and tests suggest good activity on pesticides used in grass crops such as cereals and rice. Manufacturer recommends a dose rate of 200-400 ml/ha. BREAK-THRU® has not proven phytotoxic in field trials, has a very low foaming potential and does not stabilize foams. Testing has also shown that the product reduces the amount of driftable spray particles when used with flat fan nozzles.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.960 g/cc0.0347 lb/in³
Viscosity 400 cP400 cP
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 100 °C>= 212 °F
 
Descriptive Properties
Appearanceclear to slightly yellow liquid
Content100%Active content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik TEGO® Antifoam 2-89 Emulsion
Evonik TEGO® Antifoam 2-80 Emulsion
Evonik TEGO® Antifoam 2291 Antifoam concentrate
Evonik TEGO® Antifoam 2290 Antifoam concentrate
Evonik BREAK-THRU® S 240 Surfactants

PEVONIL710 / 196914

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.