MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 201.3H HS  Nylon 6/6 - High Impact (PA 6/6 HI) Glass Fiber 13% - Heat Stable - High Impact  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Reinforced, Impact Grade

Material Notes: Glass Fiber 13% - Heat Stable - High Impact

Comments:

  • High Impact
  • Glass Fiber
  • Heat Stabilized

Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.

Information provided by RTP Company.


Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/ccASTM D792
Filler Content 13 %13 %
Water Absorption 0.90 %0.90 %24 hours at 23°C; ASTM D570
Linear Mold Shrinkage  0.0050 cm/cm
@Thickness 3.17 mm
0.0050 in/in
@Thickness 0.125 in
ASTM D955
 0.0070 cm/cm
@Thickness 6.35 mm
0.0070 in/in
@Thickness 0.250 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 82.7 MPa12000 psiASTM D638
Elongation at Break 6.0 - 8.0 %6.0 - 8.0 %ASTM D638
Modulus of Elasticity 4.48 GPa650 ksiASTM D638
Flexural Yield Strength 124 MPa18000 psiASTM D790
Flexural Modulus 3.79 GPa550 ksiASTM D790
Izod Impact, Notched 1.60 J/cm
@Thickness 3.17 mm
3.00 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 8.54 J/cm
@Thickness 3.17 mm
16.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 238 °C460 °FASTM D648
Flammability, UL94 HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in
Per testing by RTP Company; ASTM D635
 
Processing PropertiesMetricEnglishComments
Processing Temperature 274 - 293 °C525 - 560 °F
Mold Temperature 65.6 - 107 °C150 - 225 °F
Injection Pressure 103 - 124 MPa15000 - 18000 psi
 
Descriptive Properties
ColorNatural/Black

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 285H TFE 13 SI 2  Nylon 6/6 - High Impact (PA 6/6 HI) Carbon Fiber 30% - PTFE 13% - Silicone 2% - High Impact
RTP Company RTP 201 TFE 5 SI Nylon 6/6 (PA), Glass Fiber - PTFE Lubricated - Silicone Lubricated
RTP Company RTP 201 TFE 3 SI  Nylon 6/6 (PA 6/6) Glass Fiber 10% - PTFE 3% - Silicone
RTP Company RTP 201 SI 2  Nylon 6/6 (PA 6/6) Glass Fiber 10% - Silicone 2%
RTP Company RTP 201 H FR Impact-Modified Nylon 6/6 (PA), Glass Fiber - Flame Retardant

PR3850 / 63152

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.