MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Catize® DLPA-1 Inherently Conductive Polymer/metal mixtures  (discontinued **)
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic

Material Notes:

Description/Features:

  • A mixture of an Inherently Conductive Polymer and metal particles.

Applications:

  • Coil coating
  • Industrial maintenance coatings
  • Marine Coatings
  • OEM coatings
  • Rebar & Bridge Coatings
  • Fastener Coatings

As with any dry pigment, we do not recommend post adding Catize to a finished coating unless it is pre-dispersed in a suitable carrier. Catize should be added early on in the grind to ensure proper dispersion.

Disclaimer: Catize corrosion control additives are made under license of GeoTech's U.S. Pat. Nos. 5,976,419; 6,231,789; 6,440,332; 6,627,117 and other patents pending.
Catize has been tested in several finished coating formulations. It performs better on non-pretreated surfaces. Adequate cure time should be allowed prior to accelerated corrosion testing. Topcoating is not required for excellent salt spray results.

Information provided by PolyOne Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 95 - 99 %95 - 99 %
Particle Size 15 - 25 µm15 - 25 µmParticle size of the metal
 
Descriptive Properties
ColorGreen/Grey
Inherently Conductive Polymer TypeLignosulfonic acid grafted polyaniline powder
Metal Particle typeAluminum
Product FormPowder
Solvent CompatibilityMost polar solvents, preferably water miscible

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Momentive Performance Materials AC6041 Boron Nitride (BN) Powder
Avient Trilliant™ HC HC7300-0013 ESD Black Acrylonitrile Butadiene Styrene (ABS)
Avient Trilliant™ HC HC6600-0010 ESD Black Polyamide 66 (Nylon 66)
Avient Stat-Tech™ ST5220-0004 CP4D EG Black Polypropylene Impact Copolymer (PP Impact Copolymer)
Avient Stat-Tech™ OC-0307081 Black Acrylonitrile Butadiene Styrene + PC (ABS+PC)

PH1PO0006 / 43326

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.