BASF Ultramid® 7423-2 NF3001 13% Glass Filled PA66 (Dry)
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, 10% Glass Fiber Filled
Material Notes:
Ultramid 7423-2 NF3001 is an impact modified, 13% glass reinforced, heat stabilized injection molding PA6/6.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.18
g/cc
0.0426
lb/in³
ISO 1183
Linear Mold Shrinkage
0.0050
cm/cm
0.0050
in/in
ASTM Data; MD
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
90.0
MPa
13100
psi
0.2 in/min; ASTM Test
Tensile Strength, Ultimate
110
MPa
16000
psi
5mm/min; ISO 527
Elongation at Break
6.0 %
6.0 %
5mm/min; ISO 527
10 %
10 %
0.2 in/min; ASTM Test
Tensile Modulus
5.10
GPa
740
ksi
1mm/min; ISO 527
Flexural Strength
152
MPa
22000
psi
ASTM Test
Flexural Modulus
3.66
GPa
531
ksi
ASTM Test
4.70
GPa
682
ksi
ISO Data
Izod Impact, Notched
1.23
J/cm
@Thickness 3.17 mm
2.30
ft-lb/in
@Thickness 0.125 in
ASTM Test
Izod Impact, Notched (ISO)
11.0
kJ/m²
5.23
ft-lb/in²
ISO Test
Charpy Impact Unnotched
6.50
J/cm²
30.9
ft-lb/in²
ISO 179
5.50
J/cm²
@Temperature -30.0 °C
26.2
ft-lb/in²
@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched
1.00
J/cm²
4.76
ft-lb/in²
ISO 179
0.500
J/cm²
@Temperature -30.0 °C
2.38
ft-lb/in²
@Temperature -22.0 °F
ISO 179
Thermal Properties
Metric
English
Comments
Melting Point
257
°C
495
°F
10 K/min
257
°C
495
°F
ASTM Test
Deflection Temperature at 0.46 MPa (66 psi)
243
°C
469
°F
ASTM Test
256
°C
493
°F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi)
227
°C
441
°F
ASTM Test
240
°C
464
°F
ISO 75
Descriptive Properties
Color
Natural
Commercial Status
Active America
Impact Modified
Yes
Primary Processing Technique
Injection Molding
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
BASF Ultramid® 7423-2 NF3001 13% Glass Filled PA66 (Conditioned)
BASF Ultramid® 1403-2 NF3001 13% Glass Filled PA66 (Dry)
BASF Ultramid® 1703-2 BK ND3007 25% Glass Filled PA66 (Dry)
BASF Ultramid® 1503-2 BK ND3007 33% Glass Filled PA66 (Conditioned)
BASF Ultramid® 1703-2 BK ND3007 25% Glass Filled PA66 (Conditioned)
PBASF9135 / 84899
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.