MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PTS POM-270 27.0 MFI Acetal Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Information provided by Polymer Technology and Services, LLC (PTS).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.41 g/cc0.0509 lb/in³ASTM D792
Water Absorption 0.22 %0.22 %ASTM D570
Melt Flow 27 g/10 min
@Load 10.0 kg,
Temperature 220 °C
27 g/10 min
@Load 22.0 lb,
Temperature 428 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8080ASTM D785
Tensile Strength, Yield 59.3 MPa8600 psiASTM D638
Elongation at Break 38 %38 %ASTM D638
Flexural Yield Strength 85.5 MPa12400 psiASTM D790
Flexural Modulus 2.55 GPa370 ksiASTM D790
Izod Impact, Notched 0.430 J/cm
@Thickness 3.17 mm
0.806 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 158 °C316 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 110 °C230 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 160 - 180 °C320 - 356 °F
Middle Barrel Temperature 180 - 200 °C356 - 392 °F
Front Barrel Temperature 190 - 215 °C374 - 419 °F
Nozzle Temperature 190 - 215 °C374 - 419 °F
Melt Temperature 200 - 225 °C392 - 437 °F
Mold Temperature 60.0 - 100 °C140 - 212 °F
Drying Temperature 90.0 - 110 °C194 - 230 °F
Dry Time 3 - 6 hour3 - 6 hour
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Descriptive Properties
Processing Purging MaterialPolyethylene/Polystyrene

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acetal Copolymer, Unreinforced
PTS POM-90 9.0 MFI Acetal Copolymer
Envalior TEPEX® dynalite 208-C200(x)/45% Carbon - TPU Consolidated Composite Laminate
Envalior TEPEX® dynalite 201-C200(x)/45% Carbon – PA6.6 Consolidated Composite Laminate
Envalior TEPEX® dynalite 102-RGUD600(x)/47% Roving Glass – PA 6 Consolidated Composite Laminate

PZ9PU55 / 21584

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.