MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Hexcel® HexWeb® HRP - 1/4 - 5.0 Fiberglass/Phenolic Honeycomb
Categories: Ceramic; Glass; Glass Fiber; Other Engineering Material; Composite Core Material; Composite Fibers; Polymer; Thermoset; Phenolic

Material Notes: Designation: Material-Cell Size (inches)-Density
HexWeb® HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This product was developed for use at service temperatures up to 350°F. However, it is also well suited for short exposures at high temperatures. The HexWeb® HRP-series honeycomb is available in the standard hexagonal configuration, as well as in the two formale geometries - OX-Core® and Flex-Core®.

Features: High strength up to 350°F; Good insulation and dielectric properties; Good bonding surface; Readily heat formed.
Applications: HexWeb® HRP has proven to be an excellent core material for radomes, aircraft structural parts and fairings, heat shields, and other assemblies that see elevated temperature service.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0801 g/cc0.00289 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Compressive Yield Strength >= 3.65 MPa>= 530 psiBare, min
 >= 4.55 MPa>= 660 psiStabilized, min
 4.69 MPa680 psiBare, typical
 5.65 MPa820 psiStabilized, typical
Compressive Modulus 0.579 GPa84.0 ksiStabilized, typical
Shear Modulus 0.0689 GPa10.0 ksiPlate Shear, W Direction, typical
 0.138 GPa20.0 ksiPlate Shear, L Direction, typical
Shear Strength >= 1.24 MPa>= 180 psiPlate Shear, W Direction, min
 1.59 MPa230 psiPlate Shear, W Direction, typical
 >= 2.10 MPa>= 305 psiPlate Shear, L Direction, min
 2.76 MPa400 psiPlate Shear, L Direction, typical
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 177 °C350 °FHigh strength retained

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Honeywell Spectra® S--1000 650-115 Fiber
Hexcel® UHM Carbon Fiber (12,000 Filaments)
Hexcel® HexWeb® HRP/OX - 1/4 - 7.0 Fiberglass/Phenolic Honeycomb
Hexcel® HexWeb® HRP/F35 - 4.5 Nonmetallic Flex-Core Honeycomb
Hexcel® HexWeb® HRP - 3/8 - 2.2 Fiberglass/Phenolic Honeycomb

PHEXC406 / 98877

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.