MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lotte Advanced Materials Starex® EA-0640 ABS, Unreinforced
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Permanent static prevention ABS material such as LCD carrier

Information provided by Samsung Cheil Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/ccASTM D792
Melt Flow 1.8 g/10 min
@Load 5.00 kg,
Temperature 200 °C
1.8 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9696ASTM D785
Tensile Strength at Break 33.3 MPa4830 psi5 mm/min; ASTM D638
Tensile Strength, Yield 50.0 MPa7250 psi5 mm/min; ASTM D638
Elongation at Break 20 %20 %5 mm/min; ASTM D638
Tensile Modulus 1.96 GPa284 ksi5 mm/min; ASTM D638
Flexural Strength 73.5 MPa10700 psi2.8 mm/min; ASTM D790
Flexural Modulus 2.55 GPa370 ksi2.8 mm/min; ASTM D790
Izod Impact, Notched  1.86 J/cm
@Thickness 3.17 mm
3.49 ft-lb/in
@Thickness 0.125 in
ASTM D256
 1.96 J/cm
@Thickness 6.35 mm
3.67 ft-lb/in
@Thickness 0.250 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 86.0 °C
@Thickness 6.40 mm
187 °F
@Thickness 0.252 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C
@Thickness 6.40 mm
181 °F
@Thickness 0.252 in
ASTM D648
Vicat Softening Point 98.0 °C208 °FB/50; ISO R306
 100 °C212 °FB/120; ISO R306
Flammability, UL94 HB
@Thickness 1.50 - 6.00 mm
HB
@Thickness 0.0591 - 0.236 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos ABS Lustran® 2783, Extrusion Grade
Lotte Advanced Materials Starex® BM-0320 J ABS, Unreinforced
Lotte Advanced Materials Starex® CM-0140UV ABS, Unreinforced
Lotte Advanced Materials Starex® CR-0760 ABS, Unreinforced
Lotte Advanced Materials Starex® EG-0763 ABS, Unreinforced

PSAMSU726 / 146543

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.