MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Tropical Yellow Meranti Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Usual surface texture: Medium
Dimensional changes when dried lumber is subjected to variations in humidity during service: Small
Resistance to fungal decay (Heartwood in ground contact): Variable, generally Non-durable (5 to 10 years) to moderately durable
Resistance to penetration by preservatives: Extremely resistant
Common Applications: Interior joinery. Plywood

Key Words: Shorea spp.; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.460 g/cc0.460 g/ccGreen, Asian Origin
Density 0.660 g/cc0.0238 lb/in³15% Moisture Content. Density can vary by 20% or more.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 3300 N742 lb (f)Side Hardness, Green, Asian Origin
 3400 N764 lb (f)Side Hardness, 12% Moisture, Asian Origin
Modulus of Rupture 0.0552 GPa8.01 ksiStatic Bending, Green, Asian Origin
 0.0786 GPa11.4 ksiStatic Bending, 12% Moisture, Asian Origin
Flexural Modulus 9.00 GPa1310 ksiStatic Bending, Green, Asian Origin
 10.7 GPa1550 ksiStatic Bending, 12% Moisture, Asian Origin
Compressive Strength 26.8 MPa3890 psiParallel to Grain, Green, Asian Origin
 40.7 MPa5900 psiParallel to Grain, 12% Moisture, Asian Origin
Machinability 50 %50 %Medium Relative to Other Wood
Shear Strength 7.10 MPa1030 psiParallel to Grain, Green, Asian Origin
 10.5 MPa1520 psiParallel to Grain, 12% Moisture, Asian Origin
Work to Maximum Load 0.0490 J/cm³7.11 in-lb/in³Static Bending, Green, Asian Origin
 0.0650 J/cm³9.43 in-lb/in³Static Bending, 12% Moisture, Asian Origin
 
Thermal PropertiesMetricEnglishComments
Shrinkage 3.4 %3.4 %Radial Shrinkage Green to Oven Dry, Asian Origin
 8.0 %8.0 %Tangential Shrinkage Green to Oven Dry, Asian Origin
 10.4 %10.4 %Volumetric Shrinkage Green to Oven Dry, Asian Origin
 
Descriptive Properties
ColorYellow-brownUsual for heartwood

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Canadian Spruce Wood
Western White Pine
American Alaska Cedar (Yellow Cedar) Wood
American Eastern Red Cedar Wood
American Pine Wood

PTST540 / 71436

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.