MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Vitro Minerals HR-50 Recycled NanoSilica
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Vitro Minerals’ HR-50 NanoSilica is a 100% recycled, fully X-ray amorphous silica, produced by a proprietary high temperature oxidative process. It is a white, submicron-sized powder of high purity and a surface area of 20-50 m2/g. The primary particles, sized between 60 and 300 nm (0.06-0.3 µm), are spherical and form loosely agglomerated micro-clusters up to about 3 µm. HR-50 NanoSilica exceeds the requirements of ASTM C1240 and is ideally suited for use as a high reactivity pozzolan in high performance concrete, grouts, overlays, fiber cement and related demanding applications, where high early/ultimate strength and excellent durability are required. The white color is also desirable for architectural concrete applications. In addition to its pozzolanic properties, it is also effective as a thickening and thixotropic rheology control agent in cementitious and polymer-containing formulations, It can also be used as a flow aid additive in the production of industrial mineral powders.

Information provided by Vitro Minerals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Moisture Absorption at Equilibrium <= 1.0 %
@Treatment Temp. 110 °C
<= 1.0 %
@Treatment Temp. 230 °F
Free; ASMT C566
 
Component Elements PropertiesMetricEnglishComments
Loss on Ignition(%) <= 0.80 %
@Treatment Temp. 1000 °C
<= 0.80 %
@Treatment Temp. 1830 °F
ASTM D7348
Na2O <= 0.050 %<= 0.050 %ASTM C114
SiO2 >= 99.7 %>= 99.7 %ASTM C114
 
Descriptive Properties
Pozzolanic strength index (%)142ASTM C1240

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Silicon Dioxide, SiO2 (Beta Cristobalite)
Silicon Dioxide, SiO2 (Coesite)
Wacker HDK® H20 Silica
Lanxess Vulkasil® S/KG Precipitated Silica Filler for Rubber
Lanxess Vulkasil® S Precipitated Silica Filler for Rubber

CVITRO939 / 209613

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.